Material Notes:
Low Gloss, Medium Impact. Natural and colors available. Injection molding grade. Uses: General PurposeInformation provided by Engineered Polymer Solutions.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792-91
Melt Flow 7.0 g/10 min

@Load 3.80 kg,
Temperature 230 °C
7.0 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.9 MPa
5200 psi
ASTM D638
Flexural Modulus 2.21 GPa
320 ksi
ASTM D790
Izod Impact, Notched 1.87 J/cm
3.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C
203 °F
ASTM D648