Ensinger NORYL® Polyphenylene oxide (PPO)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO
Manufacturer Ensinger
Trade Name Noryl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger NORYL® Polyphenylene oxide (PPO).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
NORYL®, due to its inherent chemical composition, exhibits unusually low moisture absorption. Therefore, good electrical insulating properties are realized over a wide range of humidity and temperature conditions. Chemical attack from water, most salt solution, acids and bases is also minimal with NORYL®. The addition of glass fiber reinforcement enhances both the mechanical and thermal properties of the basic NORYL® material.Good electrical insulating properties (Due to its extremely low water absorption with values as low as 0.07%, NORYL® is an excellent electrial insulating materialLong-term dimensional stabilitySuperior impact strength (NORYL® exhibits a continuous use temperature in excess of 220°Wide ranger of UL flammability ratings from UL94 HB to UL94 V-1FDA compliance for certain gradesLight weight (NORYL®, with a density of 0.0383 lbs/in3, can be used in applications where weight is a significant consideration)Thermoformable capabilityPossesses good hydrolytic stabilityInformation Provided by Ensinger Industries, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Water Absorption 0.070 %

@Temperature 22.8 °C,
Time 86400 sec
0.070 %

@Temperature 73.0 °F,
Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 119
119
ASTM D785
Tensile Strength at Break 63.4 MPa

@Temperature 22.8 °C
9200 psi

@Temperature 73.0 °F
ASTM D638
Elongation at Break 25 %

@Temperature 22.8 °C
25 %

@Temperature 73.0 °F
ASTM D638
Tensile Modulus 2.41 GPa

@Temperature 22.8 °C
350 ksi

@Temperature 73.0 °F
ASTM D638
Flexural Strength 92.4 MPa

@Temperature 22.8 °C
13400 psi

@Temperature 73.0 °F
ASTM D790
Flexural Modulus 2.55 GPa

@Temperature 22.8 °C
370 ksi

@Temperature 73.0 °F
ASTM D790
Izod Impact, Notched 1.87 J/cm

@Temperature 22.8 °C
3.50 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Coefficient of Friction, Dynamic 0.39

@Pressure 0.276 MPa
0.39

@Pressure 40.0 psi
50 fpm
Coefficient of Friction, Static 0.32

@Pressure 0.276 MPa
0.32

@Pressure 40.0 psi
Thermal Properties Metric English Comments
CTE, linear 59.4 µm/m-°C

@Temperature -17.8 - 60.0 °C
33.0 µin/in-°F

@Temperature 0.000 - 140 °F
ASTM D696
Maximum Service Temperature, Air 104 °C
220 °F
Long Term
110 °C
230 °F
Intermittent
Deflection Temperature at 0.46 MPa (66 psi) 137 °C
279 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 123 °C
254 °F
ASTM D648
Vicat Softening Point 154 °C
310 °F
Flammability, UL94 V-1
V-1
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+17 ohm-cm

@Temperature 22.8 °C
1.00e+17 ohm-cm

@Temperature 73.0 °F
ASTM D257
Dielectric Constant 2.7

@Frequency 60.0 Hz,
Temperature 22.8 °C
2.7

@Frequency 60.0 Hz,
Temperature 73.0 °F
50% RH; ASTM D150
Dielectric Strength 19.7 kV/mm
500 kV/in
ASTM D149
Dissipation Factor 0.00070

@Frequency 60.0 Hz,
Temperature 22.8 °C
0.00070

@Frequency 60.0 Hz,
Temperature 73.0 °F
ASTM D150