Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 59.4 µm/m-°C @Temperature -40.0 - 149 °C |
33.0 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP Ertalyte® PET-P, Polyester-semi-crystalline thermoplastic, extruded (ASTM Product Data Sheet) |
|||
CTE, linear | 59.4 µm/m-°C @Temperature -40.0 - 149 °C |
33.0 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP Techtron® HPV PPS (ASTM Product Data Sheet) |
|||
CTE, linear | 59.4 µm/m-°C @Temperature 100 °C |
33.0 µin/in-°F @Temperature 212 °F |
ASTM E-831 (TMA) |
Technetics Group Amicon™ PET-P
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
CTE, linear | 59.4 µm/m-°C | 33.0 µin/in-°F | ASTM D696 |
Quantum Modified PPO - Noryl® Information provided by Quantum Advanced Engineering Plastics |
|||
CTE, linear | 59.4 µm/m-°C | 33.0 µin/in-°F | ASTM D696 |
Quantum PET Information provided by Quantum Advanced Engineering Plastics |
|||
CTE, linear | 59.4 - 101 µm/m-°C | 33.0 - 56.0 µin/in-°F | Average value: 88.3 µm/m-°C Grade Count:21 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Sheet This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Sheet". Each property range of values reported is minimum and max.. |
|||
CTE, linear | 59.4 µm/m-°C | 33.0 µin/in-°F | NOVA Chemicals Laboratory Procedure |
NOVA Chemicals Dylark® 378P12 Glass Reinforced Engineering Resin Features: Very high modulus, High heat resistance, excellent flow characteristics, excellent adhesion to urethaneApplications: Instrument panel substrates, Consoles, Cluster housings, Interior trim |
|||
CTE, linear | 59.4 µm/m-°C @Temperature 20.0 °C |
33.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
ITW Devcon Metal Repair Bronze Putty (BR), Bronze Information provided by ITW Devcon |
|||
CTE, linear | 59.4 µm/m-°C @Temperature 20.0 °C |
33.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Millennium IV Glass Filled ABS Structural Sheet Description: Structural SheetInformation provided by Spartech. |
|||
CTE, linear | 59.4 µm/m-°C @Temperature 20.0 °C |
33.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Westlake Plastics Norylux™ EN-265 Modified Polyphenylene Oxide Norylux modified PPO is a strong, engineering plastic with outstanding mechanical, thermal, and electric properties. Low moisture absorption and low thermal expansion make Norylux one of the most d.. |
|||
CTE, linear | 59.4 µm/m-°C | 33.0 µin/in-°F | Parallel to Laminate |
TriStar Ultracomp UC-200 Composite Bearing Ultracomp UC-200 - Designed for high load, high impact, slow speed, and vibratory applications. It does not absorb moisture and can operate outside and in wet environments.This family of composite m.. |
|||
CTE, linear | 59.4 µm/m-°C | 33.0 µin/in-°F | Parallel to Laminates |
TriStar Ultracomp UC-300 Composite Bearing Ultracomp UC-300 - Similar in construction to UC-200. Containing special fillers that reduce its coefficient of friction, UC-300 is designed to handle higher rotational and linear speeds.This family.. |
|||
CTE, linear | 59.4 µm/m-°C @Temperature -17.8 - 60.0 °C |
33.0 µin/in-°F @Temperature 0.000 - 140 °F |
ASTM D696 |
Ensinger NORYL® Polyphenylene oxide (PPO) NORYL®, due to its inherent chemical composition, exhibits unusually low moisture absorption. Therefore, good electrical insulating properties are realized over a wide range of humidity and temper.. |
|||
CTE, linear | 59.4 µm/m-°C | 33.0 µin/in-°F | ASTM D696 |
Diamond Polymers NPP25-0103 CF15 Conductive Copolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
CTE, linear | 59.4 µm/m-°C | 33.0 µin/in-°F | ASTM D696 |
Diamond Polymers NPP25-1111 CF15 Conductive Copolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
CTE, linear | 59.4 µm/m-°C | 33.0 µin/in-°F | |
BCC Products MB 1100 Polyurethane Foam Modeling Board MB 1100 is an Olive colored rigid closed-cell polyurethane foam tooling and modeling board. MB 1100 is low density foam of approximately 10lbs/ft3 board. Easily cut using CNC machining equipment or .. |
|||
CTE, linear | 59.4 µm/m-°C | 33.0 µin/in-°F | |
BCC Products MB 1150 Polyurethane Foam Modeling Board MB 1150 is an Avocado colored rigid closed-cell polyurethane foam tooling and modeling board. MB 1150 is low density foam of approximately 15lbs/ft3 board. Easily cut using CNC machining equipment o.. |
|||
CTE, linear | 59.4 µm/m-°C | 33.0 µin/in-°F | |
BCC Products MB 1200 Polyurethane Foam Modeling Board MB 1200 is an Apricot and/or Pink colored rigid closed-cell polyurethane foam tooling and modeling board. MB 1200 is low density foam of approximately 20lbs/ft3 board. Easily cut using CNC machining.. |
|||
CTE, linear | 59.4 µm/m-°C @Temperature 20.0 °C |
33.0 µin/in-°F @Temperature 68.0 °F |
|
Aremco Aremco-Bond™ 568 High Performance Epoxide Aluminum-Filled, 1:1, Good Bond Strength and High Thermal Conductivity. |
|||
CTE, linear | 59.4 µm/m-°C @Temperature 20.0 °C |
33.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Asahi Kasei Thermofil P-20TC-1156 20% Talc Filled, Heat Stabilized Information provided by Asahi Thermofil |
|||
CTE, linear | 59.4 µm/m-°C @Temperature 20.0 °C |
33.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Asahi Kasei Thermofil P-20TC-1161 20% Talc Filled, Heat Stabilized Information provided by Asahi Thermofil |
|||
CTE, linear | 59.4 µm/m-°C @Temperature 20.0 °C |
33.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Asahi Kasei Thermofil P-20TC-5100R 20% Talc Filled, Heat Stabilized Information provided by Asahi Thermofil |
|||
CTE, linear | 59.4 µm/m-°C @Temperature 20.0 °C |
33.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Asahi Kasei Thermofil P-20TC-5103 20% Talc Reinforced, Lubricated, Heat Stabilized Information provided by Asahi Thermofil |
|||
CTE, linear | 59.4 µm/m-°C | 33.0 µin/in-°F | |
BCC Products MB 1300 Polyurethane Foam Modeling Board MB 1300 is a Mahogany colored rigid closed-cell polyurethane foam tooling and modeling board. MB 1300 is medium low density foam of approximately 30lbs/ft3 board. Easily cut using CNC machining equi.. |
|||
CTE, linear | 59.4 µm/m-°C | 33.0 µin/in-°F | |
Aremco Aremco-Bond™ 2320 High Performance Epoxide Toughened, Unfilled, Fast-Setting, BPA Free, 2:1, High Peel & Shear Strength |
|||
CTE, linear | 59.4 µm/m-°C @Temperature 20.0 °C |
33.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
PolyOne Edgetek® MP-1000 Modified PPO - Unreinforced
(discontinued **) Data provided by PolyOne. |