Material Notes:
TECAFORM™ (Polyacetal) and TECAPRO™ SAN (Polypropylene), provide an additional safety factor in reducing incidence of bacterial contamination. The raw materials are charged with an antimicrobial additive. These silver ions are released gradually to reduce the formation of bacterial.Less bacterial contaminationReduced odor and biofilm formationDiminished formation of bacteria in equipmentActive components are harmless to humansScrubbing surface renews antimicrobial effectFDA conformity of raw material, color pigments and antimicrobial additiveTECAFORM™ SAN and TECAPRO™ SAN are ideal where continual sanitary and anti bacterial conditions are a requirement. Excellent for components in food processing equipments, bottling and canning machines, water handling and filtration equipment. Door handels and buttons in public places would benefit from reduction in transfer of bacteria. TECAPRO™ SAN is especially effective in surgical instruments, trays, work surfaces and cutting boards in medical as well as food storage and preparation areas.Information Provided by Ensinger Industries, Inc.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
Moisture Absorption at Equilibrium <= 0.30 %

@Temperature 22.8 °C
<= 0.30 %

@Temperature 73.0 °F
equilibrium, 50% RH; ISO 62
Mechanical Properties Metric English Comments
Hardness, Rockwell M 75
75
ASTM D790
Ball Indentation Hardness 144.96 MPa
21025 psi
ISO 2039/1,2
Tensile Strength, Yield 54.99 MPa
7975 psi
ASTM D638, DIN EN ISO 527
Elongation at Break 30 %
30 %
ASTM D638, ISO 527
Tensile Modulus 2.10 GPa
304 ksi
ASTM D638, ISO 527
Flexural Modulus 2.48 GPa
360 ksi
ASTM D790, ISO 178
Izod Impact Resistance NB
NB
ISO 180
Thermal Properties Metric English Comments
CTE, linear 99.0 µm/m-°C
55.0 µin/in-°F
ASTM D696, DIN 53 752, ASTM E831
Melting Point 165 °C
329 °F
DIN 53 736
Maximum Service Temperature, Air 100 °C
212 °F
Long Term
140 °C
284 °F
Sort Term
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
ISO - 75/A
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
ASTM D257, EC 93, DIN IEC 60093