Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Entec Hypro™ PP-RP12/1.5C Random Clarified Copolymer, 12 Melt Flow

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Entec Engineered Resins
Trade Name Hypro™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Entec Hypro™ PP-RP12/1.5C Random Clarified Copolymer, 12 Melt Flow.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This product is intended for injection molding applications that require fast cycle time, enhanced processability and excellent clarity. This product offers improved impact and utilizes the latest generation clarifying additive technology.Information provided by Entec
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
ASTM D955
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.0 MPa
4060 psi
ASTM D638
Elongation at Yield 11 %
11 %
ASTM D638
Flexural Modulus, 1% Secant 1070 MPa
155000 psi
ASTM D790
Izod Impact, Notched 1.49 J/cm

@Thickness 3.17 mm
2.79 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 74.0 °C
165 °F
ASTM D648