Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP AI001XXH ABS LNP* Lubricomp* AI001XXH is a compound based on ABS containing 2% Silicone. Characteristics of this grade are: Healthcare and Internally Lubricated. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DFL34EH PC LNP* LUBRICOMP* DFL34EH is a compound based on Polycarbonate containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Easy Molding, Healthcare, Wear Resistant. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 5% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 5% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Izod Impact, Notched | 1.49 J/cm @Diameter 3.17 mm |
2.79 ft-lb/in @Diameter 0.125 in |
bar, 0.010" notch radius; ASTM D256 |
Ineos Nova 5410 High Impact Polystyrene High impact, Good ESCR, Good printabilityApplications: Thermoformed containers and lids, Hot and cold beverages cups, Custom sheetProperties were determined on injection molded specimens at 23°C .. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DX94375H PC LNP* LUBRICOMP* DX94375H is a compound based on Polycarbonate resin containing Proprietary Fillers. Added features of this material include: Healthcare, Wear Resistant. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DX94375H PC (Asia Pacific) LNP* Lubricomp* DX94375H is a compound based on Polycarbonate resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL TCN8222 PPE+HIPS (Asia Pacific) PPE/HIPS unfilled 80C FR-V2 |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP PFL36 PA 6 LNP* LUBRICOMP* PFL36 is a compound based on Nylon 6 resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP PFL36 PA 6 (Asia Pacific) LNP* Lubricomp* PFL36 is a compound based on Nylon 6 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM D9065 PEI Polyetherimide blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM D9065 PEI (Asia Pacific) Polyetherimide blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RF00AS PA 66 LNP THERMOCOMP* RF00AS is a compound based on Nylon 66 resin containing 50% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP SF006 PA 12 LNP THERMOCOMP* SF006 is a compound based on Nylon 12 resin containing 30% Glass Fiber. |
|||
Izod Impact, Notched | 1.49 J/cm @Temperature -30.0 °C |
2.79 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL PPX PPX7110 PPE+PP PPE+PP blend. High Impact, Good Heat Resistance |
|||
Izod Impact, Notched | 1.49 J/cm @Temperature -30.0 °C |
2.79 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL PPX PPX7110 PPE+PP (Asia Pacific) PPE+PP blend. High Impact, Good Heat Resistance |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS (Asia Pacific) PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS (Europe-Africa-Middle East) PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP NF001 PC+ABS (Asia Pacific) LNP* Thermocomp* NF001 is a compound based on PC+ABS Blend resin containing Glass Fiber. |
|||
Izod Impact, Notched | 1.49 J/cm @Temperature 23.0 °C |
2.79 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp SF006S PA 12 LNP* Thermocomp* SF006S is a compound based on Nylon 12 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas re.. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOTUF PX06417 PA 6 LNP THERMOTUF* PX06417 is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOTUF VC006 Super Tough PA 6/6 (Asia Pacific) LNP* THERMOTUF* VC006 is a compound based on Super Tough Nylon 6/6 resin containing Carbon Fiber. Added features of this material include: High Impact. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
Unitika E-RUNG60 Ultra high-rigidity PA6, Dry Ultra high-rigidityInformation provided by Unitika Ltd. |
|||
Izod Impact, Notched | 1.49 J/cm @Thickness 3.17 mm |
2.79 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Entec Hypro™ PP-RP12/1.5C Random Clarified Copolymer, 12 Melt Flow This product is intended for injection molding applications that require fast cycle time, enhanced processability and excellent clarity. This product offers improved impact and utilizes the latest g.. |
|||
Izod Impact, Notched | 1.49 J/cm @Thickness 3.17 mm |
2.79 ft-lb/in @Thickness 0.125 in |
ASTM Test |
BASF Ultraform N 2640 Z4 UNC Q600 POM Ultraform N2640 Z4 UNC Q600 is a high toughness, elastomer-modified injection molding POM grade. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Comtuf® 618 Nylon 6, Mineral Reinforced, Impact Modified Data provided by the manufacturer, ComAlloy International Company.15% Mineral Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been i.. |
|||
Izod Impact, Notched | 1.49 J/cm @Thickness 3.18 mm |
2.79 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Thermocomp® SF-1006 Polyamide 12, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36E PC LNP LUBRICOMP* DFL36E is a compound based on Polycarbonate resin containing 30% Glass Fiber, 155 PTFE. Added features of this material include: Easy Molding, Internally Lubricated. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM-D256 |
Braskem HB0454HR HDPE Blow Molding Polyethylene Copolymer HB0454HR is a high-density polyethylene copolymer resin with average molecular weight produced by the Unipol® process. A bottle made with HB0454HR shows excellent processability, color, and superfi.. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 5% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |