Entec Hyrene® PS-HI 3/2 High Impact Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer Entec Engineered Resins
Trade Name Hyrene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Entec Hyrene® PS-HI 3/2 High Impact Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Available in North America Features: High Impact ResistanceRoHS Compliant Form: Pellets Information provided by Entec
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Melt Flow 2.9 g/10 min

@Load 5.00 kg,
Temperature 200 °C
2.9 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 23.4 MPa
3400 psi
ASTM D638
Elongation at Break 60 %
60 %
ASTM D638
Flexural Strength 38.6 MPa
5600 psi
ASTM D790
Flexural Modulus 1.88 GPa
273 ksi
ASTM D790
Izod Impact, Notched 1.28 J/cm
2.40 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 85.6 °C
186 °F
Unannealed; ASTM D648
Vicat Softening Point 101 °C
213 °F
Rate A (50°C/h), Loading 1 (10 N); ASTM D1525
Compliance Properties Metric English Comments
FDA Yes
Yes
FDA 21 CFR 177.1640