Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Epichlorohydrin Rubber (CO, ECO)

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Epichlorohydrin Rubber (CO, ECO).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CO is the ISO designation for the homopolymer and ECO is the ISO designation for the ethylene oxide copolymer. Epichlorohydrin rubber is generally damaged by chlorinated solvents, ketones, aldehydes, esters, and nitrogen-containing solvents. It is generally resistant to oil/fat/grease, ozone, and hydraulic fluid.
Physical Properties Metric English Comments
Density 1.45 - 1.60 g/cc
0.0524 - 0.0578 lb/in³
Compounded
Mechanical Properties Metric English Comments
Hardness, Shore A 40 - 90
40 - 90
Depends on compounding
Tensile Strength, Ultimate 17.0 MPa
2470 psi
Compounded Tire
Elongation at Break 150 - 500 %
150 - 500 %
Compression Set 10 %
10 %
Thermal Properties Metric English Comments
CTE, linear 648 µm/m-°C

@Temperature 20.0 °C
360 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 130 °C
266 °F
Minimum Service Temperature, Air -40.0 - -10.0 °C
-40.0 - 14.0 °F
Users viewing this material also viewed the following: