ExxonMobil ESCOREZ™ 5400 Petroleum Hydrocarbon Resin

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Adhesive
Manufacturer Exxon Chemical
Trade Name Escorez™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil ESCOREZ™ 5400 Petroleum Hydrocarbon Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Light colored cycloaliphatic hydrocarbon resin. They are designed to tackify a variety of adhesive polymers including EVA, SIS and SEBS block copolymers, natural rubber, synthetic polyisoprene, polyisobutylene, butyl rubber, metallocene polyolefins, APP and APAO. Availability: Africa & Middle East, Europe, Asia Pacific, Central America, North America and South AmericaInformation provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Viscosity 800 cP

@Temperature 160 °C
800 cP

@Temperature 320 °F
Melt; ETM 22-31
Molecular Weight 400 g/mol
400 g/mol
Mn; ETM 300-83
670 g/mol
670 g/mol
Mw; ETM 300-83
Thermal Properties Metric English Comments
Softening Point 103.4 °C
218.1 °F
ETM 22-24
Glass Transition Temp, Tg 52.0 °C
126 °F
ETM 300-90
Descriptive Properties Value Comments
Color - Initial 0.6 YI
ETM 22-13
Thermal Color Stability 6.4 YI
5 hr, 175°C, ETM 22-14