Thermal Properties Metric English Comments
Glass Transition Temp, Tg 52.0 - 58.0 °C
126 - 136 °F
ASTM D3417
NatureWorks® Ingeo™ 4060D Sealant Grade PLA
PLA (polylactide) polymer 4060D can be coextruded with other PLA resin to form a sealant layer for biaxially oriented PLA film. This resin has excellent heat seal and hot tack performance with a sea..
Glass Transition Temp, Tg 52.0 - 54.0 °C
126 - 129 °F
DMA, E
Proto3000 Objet VeroBlack FullCure870 Rigid Opaque Prototyping Polymer
Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid ..
Glass Transition Temp, Tg 52.0 - 54.0 °C
126 - 129 °F
DMA, E
Proto3000 Objet VeroClear FullCure810
Information provided by Proto3000 for their protoyping engineering services.
Glass Transition Temp, Tg 52.0 - 54.0 °C
126 - 129 °F
DMA, E
Proto3000 Objet VeroGray FullCure850 Rigid Opaque Prototyping Polymer
Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid ..
Glass Transition Temp, Tg 52.0 °C
126 °F
Unitika elitel UE3350 Polyester, Flake
Low molecular weight type UE3210, High OH typeUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as adhesives, p..
Glass Transition Temp, Tg 52.0 °C
126 °F
Ultimate Tg; DSC
Tra-Con Tra-Bond 516H03 Blush-Free Epoxy Adhesive
TRA-BOND 516H03 is a modified version of F114 yielding a higher viscosity and lower coefficient of thermal expansion. Information provided by Tra-Con Inc.
Glass Transition Temp, Tg 52.0 °C
126 °F
Ultimate Tg, 24 hrs @ 25°C
Tra-Con Tra-Duct 2902 Room Temperature Conductive Silver Epoxy Adhesive
TRA-DUCT 2902 is an electrically conducting silver-filled epoxy compound recommended for electronic bonding and sealing applications that require a combination of good mechanical and electrical prop..
Glass Transition Temp, Tg 52.0 °C
126 °F
ETM 300-90
ExxonMobil ESCOREZ™ 5400 Petroleum Hydrocarbon Resin
Light colored cycloaliphatic hydrocarbon resin. They are designed to tackify a variety of adhesive polymers including EVA, SIS and SEBS block copolymers, natural rubber, synthetic polyisoprene, poly..
Glass Transition Temp, Tg 52.0 °C
126 °F
ETM 300-90
ExxonMobil ESCOREZ™ 5600 Petroleum Hydrocarbon Resin
Light colored aromatic modified, cycloaliphatic hydrocarbon resin. Designed to tackify a variety of adhesive polymers including EVA, SIS and SEBS block copolymers and metallocene polyolefines. Avail..
Glass Transition Temp, Tg 52.0 °C
126 °F
DMA, E"
3D Systems Accura® Xtreme Plastic for SLA® Systems
For use with solid-state stereolithography (SLA®) systemsApplicationsForm, fit and function prototypesDurable AssembliesSnap fit assembliesTough enclosuresConsumer electronic componentsMaster patte..
Glass Transition Temp, Tg 52.0 °C
126 °F
DMA, E"
3D Systems Accura® Xtreme White 200 Plastic
Ultra tough white plastic to replace CNC Machined polypropylene and ABS articles FeaturesExceptionally tough and durableUsed for challenging functional assembliesUsed for snap fit assembl..
Glass Transition Temp, Tg 52.0 °C
126 °F
3M Scotch-Weld™ 2158 B/A Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 2158 B/A is a gray, two-part, high strength adhesive that chemically cures at room temperature. It has good adhesion to a variety of substrates including metals, ma..
Glass Transition Temp, Tg 52.0 - 54.0 °C
126 - 129 °F
DMA, E
Proto3000 Objet VeroWhitePlus FullCure835 Rigid Opaque Prototyping Polymer
Information provided by Proto3000 for their protoyping engineering services.