Material Notes:
Product Description: Escorene Ultra UL 7711 is a very high flow, 26.7% VA copolymer that has very good compatibility with hydrocarbon and natural tackifiers and most waxes. It is suitable for making hot melt adhesives, sealants and wax blendsAvailability: Asia Pacific, Latin America, North America and South America Additive: Antiblock: NoSlip: NoThermal Stabilizer: Yes Applications:Adhesives and SealantsIndustrial SealantsHot Melt AdhesivesWax BlendsInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.941 g/cc
0.0340 lb/in³
ExxonMobil method
Vinyl Acetate Content 26.7 %
26.7 %
ExxonMobil method
Melt Flow 400 g/10 min

@Load 2.16 kg,
Temperature 190 °C
400 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 65

@Time 15.0 sec
65

@Time 0.00417 hour
ASTM D2240
Hardness, Shore D 15

@Time 15.0 sec
15

@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break 1.38 MPa
200 psi
ASTM D638
Elongation at Break 450 %
450 %
ASTM D638
Flexural Modulus, 1% Secant 13.1 MPa
1900 psi
ASTM D790
Thermal Properties Metric English Comments
Melting Point <= 146 °C
<= 295 °F
Peak Melting Point; ExxonMobil method