ExxonMobil Exceed™ 1018KA Metallocene Polyethylene Resin (Asia Pacific Grade)

Category Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Exxon Chemical
Trade Name Exceed™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Exceed™ 1018KA Metallocene Polyethylene Resin (Asia Pacific Grade).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Exceed 1018 resins are a metallocene ethylene-hexene copolymer. Films made of Exceed 1018 resins have outstanding tensile, impact strength and puncture. These superior properties, along with excellent drawability, allow downgauging in bag application.Availability: Asia PacificAdditive:Antiblock: 5000 ppmSlip: 1000 ppm Processing Aid: YesThermal Stabilizer: YesApplications:Agricultural FilmBag in BoxBarrier Food PackagingBlown FilmBread BagsFood Packaging Form Fill and Seal PackagingFreezer FilmGeneral PackagingHeavy Duty BagsIndustrial PackagingLamination FilmMultilayer Packaging FilmOverwrap FilmPackaging FilmsPremium Trash BagsStand Up PouchesTrash BagsTrash Can Liners Information provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.918 g/cc
0.0332 lb/in³
ExxonMobil method
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Antiblock Level 5000 ppm
5000 ppm
Slip Level 1000 ppm
1000 ppm
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 9.65 MPa
1400 psi
ASTM D882
Film Tensile Strength at Yield, TD 9.65 MPa
1400 psi
ASTM D882
Film Elongation at Break, MD 500 %
500 %
ASTM D882
Film Elongation at Break, TD 600 %
600 %
ASTM D882
Elmendorf Tear Strength MD 250 g
250 g
ASTM D1922
Elmendorf Tear Strength TD 470 g
470 g
ASTM D1922
Dart Drop Test 590 g
1.30 lb
ASTM D1709
Film Tensile Strength at Break, MD 54.5 MPa
7900 psi
ASTM D882
Film Tensile Strength at Break, TD 42.7 MPa
6200 psi
ASTM D882
1% Secant Modulus, MD 186 MPa
27000 psi
ASTM D882
1% Secant Modulus, TD 193 MPa
28000 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point <= 247 °C
<= 477 °F
Peak Melting Point; ExxonMobil method
Optical Properties Metric English Comments
Haze 18 %
18 %
ASTM D1003
Gloss 39 %
39 %
45°; ASTM D2457