Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 9.65 MPa | 1400 psi | at 2% offset; ASTM D882 |
ExxonMobil Exceed™ 1018CA Premium Blown Film Resin
(discontinued **) Exceed 1018CA is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1018CA have outstanding tensile, impact strength and puncture. These superior strength .. |
|||
Film Tensile Strength at Yield, TD | 9.65 MPa | 1400 psi | at 2% offset; ASTM D882 |
ExxonMobil Exceed™ 1318CA Blown Film Resin
(discontinued **) Exceed 1318CA resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1318CA resin have outstanding tensile, impact strength and puncture. These superi.. |
|||
Film Tensile Strength at Yield, TD | 9.65 MPa | 1400 psi | at 2% offset; ASTM D882 |
ExxonMobil Exceed™ 1518CA Tough Premium Film Resin
(discontinued **) Exceed 1518CA resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1518CA resin have outstanding tensile, impact strength and puncture. These superi.. |
|||
Film Tensile Strength at Yield, TD | 9.65 MPa | 1400 psi | at 2% offset; ASTM D882 |
ExxonMobil LD 102.74 Thin Gauged Film Resin
(discontinued **) LD 102 series are homopolymer, good clarity, laundry and dry cleaning film resins capable of providing a tough film in very thin gaugesInformation provided by ExxonMobil Chemical |
|||
Film Tensile Strength at Yield, TD | 9.65 MPa | 1400 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-0225-B LDPE Clarity Film Resin
(discontinued **) Features: High optical clarityExcellent processability Applications: Produce and bakery filmLinersTextile packaging filmGeneral packaging requiring high clarity filmInformation provided by Nova Chem.. |
|||
Film Tensile Strength at Yield, TD | 9.65 MPa | 1400 psi | ASTM D882 |
Westlake LF1021 Butene Linear Low Density Polyethylene Westlake LF1021 is a butene LLDPE with excellent mechanical and downgauging advantages. It is suitable for can liners, stretch wrap, agricultural film, and blending with LDPE. This Kosher compliant .. |
|||
Film Tensile Strength at Yield, TD | 9.65 MPa | 1400 psi | |
Westlake LF2040 Hexene Linear Low Density Polyethylene Westlake LF2040 is a hexene LLDPE with excellent physical properties and heat sealing characteristics, which allow for down-gauging and blending with other materials. Typical applications include s.. |
|||
Film Tensile Strength at Yield, TD | 9.65 MPa | 1400 psi | |
Westlake LF2050 Hexene Linear Low Density Polyethylene Westlake LF2050 is a hexene LLDPE with excellent physical properties and heat sealing characteristics, which allow for down-gauging and blending with other materials. Typical applications include s.. |
|||
Film Tensile Strength at Yield, TD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil Exceed™ 1018HA Metallocene Polyethylene Resin Product Description: Exceed 1018HA is a metallocene ethylene-hexene copolymer. Films made from Exceed 1018HA have outstanding tensile, impact strength and puncture. These superior strength propertie.. |
|||
Film Tensile Strength at Yield, TD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil Exceed™ 1018KA Metallocene Polyethylene Resin Product Description: Exceed 1018 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 1018 resin have outstanding tensile, impact strength and puncture. These superior strength p.. |
|||
Film Tensile Strength at Yield, TD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil Exceed™ 1018KA Metallocene Polyethylene Resin (Asia Pacific Grade) Product Description: Exceed 1018 resins are a metallocene ethylene-hexene copolymer. Films made of Exceed 1018 resins have outstanding tensile, impact strength and puncture. These superior propertie.. |
|||
Film Tensile Strength at Yield, TD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil Exceed™ 1018KB Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1018KB is a metallocene ethylene-hexene copolymers. Films are made of Exceed 1018KB resin have outstanding tensile, impact strength and puncture. These superior strength .. |
|||
Film Tensile Strength at Yield, TD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil Exceed™ 1018LA Metallocene Polyethylene Resin Product Description: Exceed 1018 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 1018 resin have outstanding tensile, impact strength and puncture. These superior strength p.. |
|||
Film Tensile Strength at Yield, TD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil Exceed™ 1018LA Metallocene Polyethylene Resin (Asia Pacific Grade) Product Description: Exceed 1018 resins are a metallocene ethylene-hexene copolymer. Films made of Exceed 1018 resins have outstanding tensile, impact strength and puncture. These superior propertie.. |
|||
Film Tensile Strength at Yield, TD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil Exceed™ 1018MK Metallocene Polyethylene Resin Product Description: Exceed 1018 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 1018 resin have outstanding tensile, impact strength and puncture. These superior strength p.. |
|||
Film Tensile Strength at Yield, TD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil Exceed™ 1518HA Metallocene Polyethylene Resin Product Description: Exceed 1518HA is a metallocene ethylene-hexene copolymer. Films made from Exceed 1518HA have outstanding tensile, impact strength and puncture. These superior strength propertie.. |
|||
Film Tensile Strength at Yield, TD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil Exceed™ 2018KB Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 2018KB is a metallocene catalyzed ethylene-hexene copolymer. Films made from Exceed 2018KB have outstanding tensile, impact strength, and puncture. These superior strengt.. |
|||
Film Tensile Strength at Yield, TD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil LL 1001x26 Blown Film Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Film Tensile Strength at Yield, TD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil LL 1001x72 Blown Film Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Film Tensile Strength at Yield, TD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil LL 1001x74 Blown Film Resin LL1001 are butene LLDPE blown film resins having good drawdown, tensile and toughness properties.Information provided by ExxonMobil Chemical |
|||
Film Tensile Strength at Yield, TD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil LL 1001x76 Blown Film Resin LL1001 are butene LLDPE blown film resins having good drawdown, tensile and toughness properties.Information provided by ExxonMobil Chemical |
|||
Film Tensile Strength at Yield, TD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil LLDPE LL 1001X26 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Film Tensile Strength at Yield, TD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil LLDPE LL 1001X31 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Film Tensile Strength at Yield, TD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil LLDPE LL 1001X72 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Film Tensile Strength at Yield, TD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil LLDPE LL 1001X74 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Film Tensile Strength at Yield, TD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil LLDPE LL 1001X76 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Film Tensile Strength at Yield, TD | 9.65 MPa | 1400 psi | ASTM D882 |
Dow FLEXOMER™ ETS-9064 NT 7, 0.8 mil Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ ETS-9064 NT 7 is intended for use in single of multi-layer blown-film constructions or thick sheets. Films extruded from ETS-9064 NT 7 have a high tear strength, high impact strength, an.. |
|||
Film Tensile Strength at Yield, TD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil Exceed™ 1018HA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1018HA is a metallocene ethylene-hexene copolymers. Films are made of Exceed 1018HA have outstanding tensile, impact strength and puncture. These superior strength proper.. |
|||
Film Tensile Strength at Yield, TD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil Exceed™ 1018JA Metallocene Polyethylene Resin Product Description: Exceed 1018 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 1018 resin have outstanding tensile, impact strength and puncture. These superior strength p.. |
|||
Film Tensile Strength at Yield, TD | 9.65 MPa | 1400 psi | ASTM D882 |
ExxonMobil Exceed™ 3527PA Metallocene Polyethylene Resin Product Description: Exceed 3527PA is a metallocene ethylene-hexene copolymer. Films made from Exceed 3527PA have high modulus and outstanding tensile, impact and puncture resistance properties. The.. |