Material Notes:
Product Description: Exceed 1327HA is a metallocene ethylene-hexene copolymer. Films made from Exceed 1327HA resin have excellent tensile, impact strength and puncture. These superior strength properties, along with excellent drawability, allow downgauging in bag applications.Availability: Africa & Middle East, Asia Pacific and EuropeAdditive:Antiblock: NoSlip: No Processing Aid: Yes Thermal Stabilizer: Yes Applications: Bag in a BoxBarrier Food Packaging Blown Film Food packagingForm Fill and Seal PackagingGeneral Packaging Heavy Duty BagsLabel Film Multilayer Packaging Film Overwrap FilmPackaging FilmsPremium Trash BagsProduce Bags Shrink FilmStand Up PouchesTrash Bags Information provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.927 g/cc
0.0335 lb/in³
ExxonMobil method
Melt Flow 1.3 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.3 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 12.4 MPa
1800 psi
ASTM D882
Film Tensile Strength at Yield, TD 13.8 MPa
2000 psi
ASTM D882
Film Elongation at Break, MD 600 %
600 %
ASTM D882
Film Elongation at Break, TD 730 %
730 %
ASTM D882
Elmendorf Tear Strength MD 170 g
170 g
ASTM D1922
Elmendorf Tear Strength TD 480 g
480 g
ASTM D1922
Dart Drop Test 140 g
0.309 lb
ASTM D1709
Film Tensile Strength at Break, MD 57.9 MPa
8400 psi
ASTM D882
Film Tensile Strength at Break, TD 49.6 MPa
7200 psi
ASTM D882
1% Secant Modulus, MD 303 MPa
44000 psi
ASTM D882
1% Secant Modulus, TD 331 MPa
48000 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point <= 252 °C
<= 486 °F
Peak Melting Point; ExxonMobil method
Optical Properties Metric English Comments
Haze 40 %
40 %
ASTM D1003
Gloss 21 %
21 %
45°; ASTM D2457