ExxonMobil Jayflex™ L911P Plasticizer

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Exxon Chemical
Trade Name Jayflex™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Jayflex™ L911P Plasticizer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Appearance: Clear and FreeAvailability: North AmericaCAS Number: 685151-43-5Information provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.958 - 0.964 g/cc
0.0346 - 0.0348 lb/in³
BRCP 4843
Maximum Moisture Content 0.10
0.10
BRCP 5053
Descriptive Properties Value Comments
Acidity <0.015%
as phthalic acid, BRCCP 4625
Color <50
Platinum Cobalt, BRCP 4273
Ester Content >99.6%
BRCP 4360