Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Label-Lyte™ 50ML580 OPP Film

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Exxon Chemical
Trade Name Label-Lyte™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Label-Lyte™ 50ML580 OPP Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A metalized, surface printable OPP film designed for pressure sensitive applications where high-sheen metalized appearance and high-speed press performance are desired. The proprietary top-coated metal print surface is designed for excellent print receptivity for a broad base of ink chemistries. The coating on the print surface Is similar to that on LL539. 50ML580 is compatible with UV flexo and solvent-based gravure systems. The adhesive surface is uncoated and may require base roll treatment.Availability: Europe, Latin America, North America and South AmericaKey Features: Excellent coated metal appearanceExcellent unconverted shelf life of coated metal print surfaceExcellent “in-to-out” blocking resistanceExcellent stiffness for automatic label dispensingApplications: Beverage, AlcoholicBeverage, Carbonated Beverage, Mineral Waters Health and Beauty CareHousehold and Detergents Uses: Pressure Sensitive LabelsProcessing Method: Conventional Offset Lithography, Solvent Flexographic Printing, Solvent Rotogravure Printing, Surface Print Unsupported, UV Flexographic Printing, UV Letterpress Printing, UV Offset Lithography Printing, UV Screen Printing and Water-based Flexographic PrintingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
ExxonMobil Method
Coating Weight 45.4 g/m²
28.4 lb/ream
ExxonMobil Method
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 175 %
175 %
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Film Elongation at Break, TD 50 %
50 %
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Modulus of Elasticity 2.10 GPa
305 ksi
MD; ExxonMobil Method
3.50 GPa
508 ksi
TD; ExxonMobil Method
Film Tensile Strength at Break, MD 120 MPa
17400 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 270 MPa
39200 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Thermal Properties Metric English Comments
Shrinkage, MD 3.5 %

@Temperature 135 °C,
Time 432 sec
3.5 %

@Temperature 275 °F,
Time 0.120 hour
ExxonMobil Method
Shrinkage, TD 3.0 %

@Temperature 135 °C,
Time 432 sec
3.0 %

@Temperature 275 °F,
Time 0.120 hour
ExxonMobil Method
Optical Properties Metric English Comments
Gloss 80 %
80 %
45°, Print Surface; ExxonMobil Method
Descriptive Properties Value Comments
Yield 15200 in2/lb
Users viewing this material also viewed the following: