Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.10 - 8.27 GPa | 305 - 1200 ksi | Average value: 5.57 GPa Grade Count:57 |
Overview of materials for Polycarbonate, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | Youngs Modulus, ASTM D638, 10%/min. |
EVALCA EVAL® LC-E105A Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 44 mol % Ethylene.Data provided by EVALCA. Applications: Cast film, melt phase forming, solid phase pressure forming, tubes, coex coating. EVOH is used in packaging applications because of its out.. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | Youngs Modulus, ASTM D638, 10%/min. |
EVALCA EVAL® LC-E151B Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 44 mol % Ethylene.Data provided by EVALCA. Applications: Melt phase forming, solid phase pressure forming, blow molding, tubes EVOH is used in packaging applications because of its outstanding gas.. |
|||
Modulus of Elasticity | 2.10 - 7.20 GPa @Temperature 60.0 - 150 °C |
305 - 1040 ksi @Temperature 140 - 302 °F |
Average value: 4.04 GPa Grade Count:2 |
Overview of materials for Nylon 12, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 33LL247 OPP Film Product Description: A super white opaque, high gloss, caviated BOPP film designed for use in reel-fed warp-around labeling applications where superior graphics are desired.Availability: Africa & Mi.. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 38LW280 OPP Film Product Description: A super white opaque slip controlled, biaxially oriented polypropylene film, metalized on one side. Designed for use in reel-fed wrap-around applications, where outstanding meta.. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 47LL247 OPP Film Product Description: A super white opaque, high gloss, cavitated BOPP film designed for use in reel-fed wrap-around labeling applications where superior graphics are desired.Availability: Africa & M.. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Metallyte™ 38ICE M OPP Film Product Description: A coextruded super white opaque, low density, biaxially oriented polypropylene film, metalized on one side. This film is designed for HFFS applications, heat seal or cold seal.A.. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Metallyte™ 38MW480 OPP Film Product Description: A super white opaque biaxially oriented polypropylene film, metalized on one side.Availability: Africa & Middle East, Asia Pacific and EuropeKey Features: Outstanding opacity an.. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Oppalyte™ 30MW648 OPP Film Product Description: A high speed super white opaque, biaxially oriented polypropylene film coated one side acrylic, one side very low temperature seal (VTLS) coating. VLTS coating provides an excel.. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Oppalyte™ 35MW647 OPP Film Product Description: A super white opaque biaxially oriented polypropylene film acrylic coated two sides. Provides outstanding performances on all types of packaging machines.Availability: Africa & .. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Oppalyte™ 38ICE OPP Film Product Description: A coextruded white opaque, low density, biaxially oriented polypropylene film. This film is designed for the ice cream applications, and is suitable for heat seal and cold seal .. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Oppalyte™ 38MW247 OPP Film Product Description: A super white opaque biaxially oriented polypropylene film. It is designed for use in cold seal applications where superior optics and graphics are desired.Availability: Africa .. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Oppalyte™ 40MW648 OPP Film Product Description: A high speed super white opaque, biaxially oriented polypropylene film coated one side acrylic, one side very low temperature seal (VLTS) coating. VLTS coating provides an excel.. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Oppalyte™ 45MW647 OPP Film Product Description: A super white opaque biaxially oriented polypropylene film acrylic coated two sides. Acrylic provides excellent aroma barrier and excellent support for printing. The film provid.. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Oppalyte™ 47MW247 OPP Film Product Description: A super white opaque biaxially oriented polypropylene film. It is designed for use in cold seal applications where superior optics and graphics are desired.Availability: Africa .. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | Conditioned; ISO 178 |
Addiplast Addilene H 490 M10S Flame Retardant Polypropylene Flame retardant, mineral filled, with halogensInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | Conditioned; ISO 178 |
Addiplast Addilene J 690 RM20F Flame Retardant Polypropylene, 20% Mineral Filled Flame retardant, mineral filled, with halogens, impact resistantInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | ISO 178 |
Addiplast Addilene PMD 50213 Polypropylene Copolymer Mineral reinforced, improved scratch resistanceInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | ISO 178 |
Addiplast Addilene J 520 T30 Polypropylene Copolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | ISO 178 |
Addiplast Addinyl PMD 20143 Nylon 6 High impact resistanceInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Oppalyte™ 33ICE OPP Film Product Description: Coextruded white opaque, low density, biaxially oriented polypropylene film. This film is designed for the ice cream applications, and is suitable for heat seal and cold seal on.. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Oppalyte™ 40MW647 OPP Film Product Description: A super white opaque, biaxially oriented polypropylene film acrylic coated two sides. Provides outstanding performance on all types of packaging machines.Availability: Africa & .. |