Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.10 GPa | 305 ksi | DIN 53457 |
Ineos Nova S-3401 Medium Impact Compact Polystyrene
(discontinued **) Impact polystyrene with good flow characteristics and a high elongation. Generally used for applications where a tough material is required. The material is provided with external lubricate to imp.. |
|||
Modulus of Elasticity | 2.10 - 8.27 GPa | 305 - 1200 ksi | Average value: 5.57 GPa Grade Count:57 |
Overview of materials for Polycarbonate, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Modulus of Elasticity | 2.10 - 7.20 GPa @Temperature 60.0 - 150 °C |
305 - 1040 ksi @Temperature 140 - 302 °F |
Average value: 4.28 GPa Grade Count:3 |
Overview of materials for Nylon 12 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en.. |
|||
Modulus of Elasticity | 2.10 - 7.20 GPa @Temperature 60.0 - 150 °C |
305 - 1040 ksi @Temperature 140 - 302 °F |
Average value: 4.04 GPa Grade Count:2 |
Overview of materials for Nylon 12, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | |
Lehmann & Voss LUVOCOM® 1500-8299 Polysulfone, with PTFE, lubricant modified Applications: Isotropic shrinkage characteristics.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precision parts, high continuous use temperature.Control disks, ca.. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | ASTM D638 |
Spartech Royalite R21M General Purpose ABS Resin Data provided by the manufacturer. A general-purpose ABS resin with high impact strength, R-21M is a popular choice for a variety of products, from bicycle helmets and carrying cases to portable ta.. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 33LL247 OPP Film Product Description: A super white opaque, high gloss, caviated BOPP film designed for use in reel-fed warp-around labeling applications where superior graphics are desired.Availability: Africa & Mi.. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 38LL247 OPP Film Product Description: A super white opaque, high gloss, cavitated BOPP film designed for use in reel-fed wrap-around labeling applications where superior graphics are desired.Availability: Africa & M.. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 38LW280 OPP Film Product Description: A super white opaque slip controlled, biaxially oriented polypropylene film, metalized on one side. Designed for use in reel-fed wrap-around applications, where outstanding meta.. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 47LL247 OPP Film Product Description: A super white opaque, high gloss, cavitated BOPP film designed for use in reel-fed wrap-around labeling applications where superior graphics are desired.Availability: Africa & M.. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 47LTL247 OPP Film Product Description: A super white opaque, high gloss, cavitated BOPP film designed for use in reel-fed wrap-around labeling applications where superior graphics are desired. 47LTL247 with supplied .. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | MD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 50ML580 OPP Film Product Description: A metalized, surface printable OPP film designed for pressure sensitive applications where high-sheen metalized appearance and high-speed press performance are desired. The prop.. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Metallyte™ 38MW480 OPP Film Product Description: A super white opaque biaxially oriented polypropylene film, metalized on one side.Availability: Africa & Middle East, Asia Pacific and EuropeKey Features: Outstanding opacity an.. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Oppalyte™ 35MW647 OPP Film Product Description: A super white opaque biaxially oriented polypropylene film acrylic coated two sides. Provides outstanding performances on all types of packaging machines.Availability: Africa & .. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Oppalyte™ 38MO447 OPP Film Product Description: A coextruded white opaque, low density, biaxially oriented polypropylene film, heat sealable on the inside. The treated layer must be printed and varnished to provide the necess.. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Oppalyte™ 38MW247 OPP Film Product Description: A super white opaque biaxially oriented polypropylene film. It is designed for use in cold seal applications where superior optics and graphics are desired.Availability: Africa .. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Oppalyte™ 47MW247 OPP Film Product Description: A super white opaque biaxially oriented polypropylene film. It is designed for use in cold seal applications where superior optics and graphics are desired.Availability: Africa .. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | Conditioned; ISO 178 |
Addiplast Addilene H 490 M10S Flame Retardant Polypropylene Flame retardant, mineral filled, with halogensInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | ISO 178 |
Addiplast Addilene H 555 Y7 Polypropylene Homopolymer Good surface appearance, high temperature resistanceInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | ISO 178 |
Addiplast Addilene PMD 50213 Polypropylene Copolymer Mineral reinforced, improved scratch resistanceInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | ISO 178 |
Addiplast Addilene J 520 T30 Polypropylene Copolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | ISO 178 |
Addiplast Addinyl PMD 20143 Nylon 6 High impact resistanceInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Oppalyte™ 33MW247 OPP Film Product Description: A super white opaque biaxially oriented polypropylene film. It is designed for use in cold seal applications where superior optics and graphics are desired.Availability: Africa .. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | TD; ExxonMobil Method |
ExxonMobil Oppalyte™ 40MW647 OPP Film Product Description: A super white opaque, biaxially oriented polypropylene film acrylic coated two sides. Provides outstanding performance on all types of packaging machines.Availability: Africa & .. |
|||
Modulus of Elasticity | 2.10 GPa | 305 ksi | ISO 178 |
Addiplast Addilene H 552 Y7 Polypropylene Homopolymer Good surface appearance, high temperature resistanceInformation provided by Addiplast. |