ExxonMobil Mytex™ AS33L(W)-06

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Exxon Chemical
Trade Name Mytex™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Mytex™ AS33L(W)-06.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Talc and rubber modified polypropylene for automotive exterior applications. Offers excellent flow properties and good balance of high stiffness and impact performance.Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.970 g/cc
0.0350 lb/in³
Melt Flow 28 g/10 min

@Load 2.16 kg,
Temperature 230 °C
28 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Mechanical Properties Metric English Comments
Hardness, Rockwell R 50
50
Tensile Strength, Yield 20.0 MPa
2900 psi
2 in/min; LAB032
Flexural Modulus 1.400 GPa
203.1 ksi
1% tangent, 0.05 in/min.; LAB033
Izod Impact, Notched 5.50 J/cm
10.3 ft-lb/in
LAB034
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
LAB036