ExxonMobil OPPalyte® 30 HM OPP Film

Category Polymer , Film , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Exxon Chemical
Trade Name OPPalyte®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil OPPalyte® 30 HM OPP Film.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: White opaque OPP film with a proprietary cavitated core. Designed for cold seal applications and is used as a surface print, monoweb, or as the inside web of a lamination. Availability: Latin America, North America and South AmericaKey Features:Excellent stiffness an flex resistanceOutstanding opacityBright white appearanceVery good moisture barrierExcellent print performance for flexographic and rotogravure printingThe treated print layer provides very good ink adhesionThe treated cold seal layer provides exceptional cold seal adhesion, with very good adhesion to synthetic cold sealsThe treated cold seal layer allows for back-side printing with FDA approved inksFeatures:Light BarrierMoisture BarrierApplications: BakeryBiscuits/Cookie/CrackersConfectionery, Chocolate Confectionery, Gum Confectionery, SugarIce Cream Uses:HFFS Flexible PackagingProcessing Method: Cold Seal Adhesive, Inner Web Adhesive Lamination, Inner Web Extrusion Lamination, Solvent Flexographic Printing, Solvent Rotogravure Printing, Surface Print Unsupported and Water-based Flexographic PrintingInformation provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Water Vapor Transmission 5.90 g/m²/day
0.380 g/100 in²/day
38°C, 90% RH; ExxonMobil
Thickness 33.0 microns
1.30 mil
ExxonMobil
Coating Weight 20.0 g/m²
12.5 lb/ream
ExxonMobil
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 74.463 MPa
10800 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil
Film Tensile Strength at Break, TD 179.26 MPa
26000 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil
Thermal Properties Metric English Comments
Shrinkage, MD 5.0 %
5.0 %
at 275°F; ExxonMobil
Shrinkage, TD 5.0 %
5.0 %
at 275°F; ExxonMobil
Optical Properties Metric English Comments
Gloss 65 %
65 %
45°; ExxonMobil
Transmission, Visible 30 %
30 %
ExxonMobil Method
Descriptive Properties Value Comments
Opacity 80%
Wetting Tension 0.8 receding COS theta
cold seal surface
0.9 receding COS theta
print surface
Yield 34500 in2/lb