Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 91.1 °C | 196 °F | ASTM D648 |
RheTech Products HP800-706UV 20% Talc Reinforced High Performance Polypropylene Copolymer, Scratch Resistant, UV Stabilized, Impact Modified, SWB White Applications: Interior trim/Instrument panel componentsA/B pillarsGlove box doorsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 91.1 - 146 °C | 196 - 295 °F | Average value: 137 °C Grade Count:16 |
Overview of materials for Polycarbonate, Stainless Steel Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Stainless Steel Fiber". Each property range of values reported is minimum and maximum val.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 91.1 °C | 196 °F | Unannealed; ASTM D648 |
Global PP-2512-H Polypropylene Block Copolymer Description-opacity, medium to high stiffness, high impact strength at low temperatureApplications-special for wire & cable, telecom insulationInformation provided by Global Polymers Corporation. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 91.1 °C | 196 °F | ISO 75-2/Bf |
ExxonMobil Exxtral™ CNT 001W Performance Polyolefin Product Description: High impact, medium melt flow rate copolymer, colored black. Particularly suitable for injection molded automotive interior & exterior applications. Availability: North America .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 91.1 °C | 196 °F | ASTM D648 |
ExxonMobil PP143KNE1 Polypropylene Homopolymer Product Description: A high impact copolymer resin designed consumer and industrial applications.Availability: North America Features:Good ColorabilityGood Dimensional StabilityGood Mold ReleaseGoo.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 91.1 °C | 196 °F | ASTM D648 |
Aclo Accuguard Polypropylene HP0362V0CSL Homopolymer Flame Retardant Copper Stabilized |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 91.1 °C | 196 °F | ASTM D648 |
Aclo Accucomp SAN SAN900L |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 91.1 °C | 196 °F | ASTM D648 |
Aclo Accuguard Polypropylene HPN469V2CSL Homopolymer Non-Halogenated Copper Stabilized |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 91.1 °C | 196 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® ABS 922 NAT Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc. |