Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Santoprene® 291-75B150 Thermoplastic Vulcanizate

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer Exxon Chemical
Trade Name Santoprene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Santoprene® 291-75B150 Thermoplastic Vulcanizate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PC, ABS, PC/ABS, ASA and PMMA for applications where hard/oft combinations are required. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It is polyolefin based and completely recyclable.Key Features:Designed for excellent adhesion to PC, ABS, PC/ABS, ASA and PMMA (cold insert or 2K [two-shot] molding).Broad processing window in injection molding.Recommended for applications requiring superior part surface appearance.UL listed, EU and China RoHS compliant.Applications:Automotive-Plugs, Bumpers, Grommets, ClipsConsumer-Floor Care, Kitchen Tools, Power Tools, Writing InstrumentsConsumer ApplicationsSeals and GasketsSoft Touch GripsUses:Appliance ComponentsAppliancesAutomotive ApplicationsAutomotive Under the HoodBondingCell PhonesConsumer ApplicationsEyeglass FramesFlexible GripsKitchenwareLiving HingesSealsSporting GoodsStrain ReliefsTie-LayerWhite Goods & Small AppliancesProcessing Method: Coextrusion, Injection Molding and Multi Injection Molding Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaInformation provided by ExxonMobil Chemical.
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792 and ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 74

@Time 15.0 sec
74

@Time 0.00417 hour
2 mm; ISO 868
Tensile Strength at Break 11.7 MPa
1700 psi
Across Flow; ASTM D412 and ISO 37
Tensile Stress 3.20 MPa

@Strain 100 %
464 psi

@Strain 100 %
Across Flow; ASTM D412 and ISO 37
Elongation at Break 570 %
570 %
Across Flow; ASTM D412 and ISO 37
Tear Strength 46.0 kN/m
262 pli
Across Flow, Die C; ASTM D624
46.0 kN/m
262 pli
Across Flow, Method Bb, Angle (Nicked); ISO 34-1
Compression Set 37 %

@Temperature 23.0 °C,
Time 79200 sec
37 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395B Type 1 and ISO 188 Type A
68 %

@Temperature 70.0 °C,
Time 79200 sec
68 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395B Type 1 and ISO 188 Type A
Thermal Properties Metric English Comments
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
UL File Number - E80017
HB

@Thickness 2.10 mm
HB

@Thickness 0.0827 in
Descriptive Properties Value Comments
Change in Tensile Strength in Air -8.0%
ASTM D573, 100°C, 168 hr
Change in Ultimate Elongation in Air -11%
ASTM D573, 100°C, 168 hr