Material Notes:
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Specific Gravity 1.67 g/cc
1.67 g/cc
ASTM D792
Linear Mold Shrinkage 0.0020 cm/cm

@Thickness 3.175 mm
0.0020 in/in

@Thickness 0.1250 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 125 MPa
18200 psi
ASTM D638
Flexural Strength 178 MPa
25800 psi
ASTM D790
Flexural Modulus 10.51 GPa
1525 ksi
ASTM D790
Izod Impact, Notched 0.801 J/cm
1.50 ft-lb/in
ASTM D256