Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Fainplast Compounds HAX HF 4221 Halogen Free PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Fainplast Compounds
Trade Name HAX
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds HAX HF 4221 Halogen Free PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General purpose
Physical Properties Metric English Comments
Density 1.47 - 1.51 g/cc
0.0531 - 0.0546 lb/in³
IEC 60811
Melt Index of Compound 6.0 g/10 min

@Load 21.6 kg,
Temperature 150 °C
6.0 g/10 min

@Load 47.6 lb,
Temperature 302 °F
Fainplast
Mechanical Properties Metric English Comments
Hardness, Shore D 47 - 53
47 - 53
IEC 60811
Tensile Strength at Break 12.0 MPa
1740 psi
IEC 60811
Elongation at Break 180 %
180 %
IEC 60811
Thermal Properties Metric English Comments
Oxygen Index 42 %
42 %
ISO 4589
Electrical Properties Metric English Comments
Volume Resistivity 6.00e+14 ohm-cm

@Temperature 20.0 °C
6.00e+14 ohm-cm

@Temperature 68.0 °F
ASTM D257
Copyright © lookpolymers.com All Rights Reserved