Fainplast Compounds HGK 83/1 Flexible PVC, Sheathing for High Temperatures Lead Free

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Fainplast Compounds
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds HGK 83/1 Flexible PVC, Sheathing for High Temperatures Lead Free.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Operating temperature 105°C
Physical Properties Metric English Comments
Density 1.43 - 1.47 g/cc
0.0517 - 0.0531 lb/in³
ISO R 1184
Mechanical Properties Metric English Comments
Hardness, Shore A 81 - 85
81 - 85
ISO R 868
Tensile Strength at Break >= 12.0 MPa
>= 1740 psi
ISO R 527
Elongation at Break >= 290 %
>= 290 %
ISO R 527
Thermal Properties Metric English Comments
Brittleness Temperature -30.0 °C
-22.0 °F
Cold Flex; ISO 458/2
Descriptive Properties Value Comments
Thermal Stability (minutes) 180
CEI 20-34/3-2