Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Fainplast Compounds Hax™ HFX 505/2 Crosslinkable HFFR Cable Compound

Category Polymer , Thermoplastic , Polyolefin , Polyolefin, Wire/Cable Grade
Manufacturer Fainplast Compounds
Trade Name Hax™ HFX
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds Hax™ HFX 505/2 Crosslinkable HFFR Cable Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Sheathing; InsulationInformation provided by Fainplast Compounds
Physical Properties Metric English Comments
Density 1.48 - 1.52 g/cc
0.0535 - 0.0549 lb/in³
ISO 1183
Melt Flow 3.0 g/10 min

@Load 21.6 kg,
Temperature 150 °C
3.0 g/10 min

@Load 47.6 lb,
Temperature 302 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 44 - 50
44 - 50
ISO 868
Tensile Strength 13.5 MPa
1960 psi
Crosslinked specimen; ISO 527
Elongation at Break 190 %
190 %
Crosslinked specimen; ISO 527
Thermal Properties Metric English Comments
Oxygen Index 38 %
38 %
ISO 4589
Electrical Properties Metric English Comments
Volume Resistivity >= 6.00e+14 ohm-cm
>= 6.00e+14 ohm-cm
ASTM D257
Processing Properties Metric English Comments
Processing Temperature 120 - 200 °C
248 - 392 °F
Shelf Life 3.00 Month

@Temperature 30.0 °C
3.00 Month

@Temperature 86.0 °F
Moisture absorption after extended storage