Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | <= 105 µm | <= 105 µm | 37%; Geon® DFT 1466; Internal Method |
PolyOne Geon™ Specialty Suspension Atlas E 43 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® Atlas E 43 is a non-chain modified ultra-high molecular weight homopolymer specialty suspension resin intended for use in high strength extruded parts. It improves the physical properties, fo.. |
|||
Particle Size | <= 105 µm | <= 105 µm | 6.9%; Geon® DFT 1466; Internal Method |
PolyOne Geon™ Specialty Suspension Atlas E 46 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® Atlas E 46 is high molecular weight homopolymer specialty suspension resin intended for use in high strength extruded parts. It improves the physical performance of end application for instan.. |
|||
Particle Size | <= 105 µm | <= 105 µm | 14.8%; Geon® DFT 1466; Internal Method |
PolyOne Geon™ Specialty Suspension Atlas S140 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® Atlas S140 is high molecular weight homopolymer specialty suspension resin intended for use in high strength extruded parts. It improves the physical performance of end application for intsan.. |
|||
Particle Size | <= 105 µm | <= 105 µm | 40%; Geon® DFT 1466; Internal Method |
PolyOne Geon™ Specialty Suspension CG E 24 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® CG E24 is a homopolymer specialty suspension resin intended for use in controlling gloss and transparency of injection molded, extruded or plastisol parts. This resin provides low surface glo.. |
|||
Particle Size | <= 105 µm | <= 105 µm | 16%; Geon® DFT 1466; Internal Method |
PolyOne Geon™ Specialty Suspension CG E 44 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® CG E44 is a homopolymer specialty suspension resin intended for use in lowering the gloss of extruded or plastisol parts. This resin provides low surface gloss and texturing effects for flexi.. |
|||
Particle Size | <= 105 µm | <= 105 µm | 14%; Geon® DFT 1466; Internal Method |
PolyOne Geon™ Specialty Suspension Impel S100 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® Impel S100 is a homopolymer specialty suspension resin intended for use in highly plasticized extrusion and injection molding formulations. It gives superior plasticizer absorption properties.. |
|||
Particle Size | <= 105 µm | <= 105 µm | |
Ferro CF 7575 Display Device Glass Type: Pb-Zn-B (Composite) Typical Powder Form: VSD Typical Application: Seal (Devitrified) Ferro's display sealing glasses and dielectrics are low-temperature lead glasses suitable for herm.. |
|||
Particle Size | <= 105 µm | <= 105 µm | |
Ferro EG 4010 Display Device Glass Type: Pb-B-AL Typical Powder Form: VSD Typical Application: Dielectric Ferro's display sealing glasses and dielectrics are low-temperature lead glasses suitable for hermetic sealing and pas.. |
|||
Particle Size | <= 105 µm | <= 105 µm | |
Ferro EG 4020 Display Device Glass Type: Pb-B-AL Typical Powder Form: VSD Typical Application: Dielectric Ferro's display sealing glasses and dielectrics are low-temperature lead glasses suitable for hermetic sealing and pas.. |
|||
Particle Size | <= 105 µm | <= 105 µm | DSD Powder |
Ferro IX 2443 Passivation Glasses - High Voltage (Zn-B-Silicates) Typical Powder Form: RWG, DSD Zinc-Boro-Silicate passivation glasses are used for hermetic passivation of high voltage diodes, thyristors, and transistors. They provide high junction temperatures a.. |
|||
Particle Size | <= 105 µm | <= 105 µm | |
Ferro IX 2683 Passivation Glasses - High Voltage (Zn-B-Silicates) Typical Powder Form: DSD Zinc-Boro-Silicate passivation glasses are used for hermetic passivation of high voltage diodes, thyristors, and transistors. They provide high junction temperatures and ca.. |
|||
Particle Size | 105 - 135 µm | 105 - 135 µm | Laser Light Scattering Method; LSY-QB-ID016 |
LG Chemical Lutex 703 SBR Latex Description: Binding Force, Ink set off, Post Treatment Properties, Coater RunnabilityApplication: Art Paper, Paperboard-Single, Pre-Rod, Blade Coater, Adhesive coated paper and Carpet back-coating .. |
|||
Particle Size | 105 µm | 105 µm | Average Mean |
SPHERE ONE EXTENDOSPHERESâ„¢ FM-1 Hollow Spheres EXTENDOSPHERESâ„¢FM-1 ceramic hollow spheres are a low-density functional additive for disc brake pads, truck and train blocks, clutch facings and other friction materials. They are compatible wi.. |
|||
Particle Size | 105 µm | 105 µm | 95th% |
3M A20/1000 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 105 µm | 105 µm | 95th% |
3M H20/1000 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 105 µm | 105 µm | 90th% |
3M K15 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 105 µm | 105 µm | Effective Top Size |
3M K20 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 105 µm | 105 µm | Effective Top Size |
3M K25 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |