Material Notes:
Glass Type: Si-MG-Al Typical Powder Form: MVG Typical Application: Sintering Aid / Glaze Ferro offers a wide range of compositions for specialty applications including sintering aids used in the glass-phase bonding of refractory ceramic oxides and glass-ceramics for substrates.Information provided by Ferro Corporation
Physical Properties Metric English Comments
Density 2.70 g/cc
0.0975 lb/in³
Particle Size 5.0 µm
5.0 µm
50% of particles
<= 25 µm
<= 25 µm
Thermal Properties Metric English Comments
CTE, linear 5.00 µm/m-°C
2.78 µin/in-°F
at Set Pt.
4.65 µm/m-°C

@Temperature 260 °C
2.58 µin/in-°F

@Temperature 500 °F
Softening Point >= 1000 °C
>= 1830 °F
Transformation Temperature 620 °C
1150 °F
Processing Properties Metric English Comments
Processing Temperature 1300 °C
2370 °F
Typical Firing Temperature