Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.90 GPa @Temperature 23.0 °C |
711 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB SCANMID 6 B60 Nylon 6, Modified Information provided by Polykemi AB |
|||
Flexural Modulus | 4.90 GPa | 711 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® HFD4472 PC (Asia Pacific) Lexan* HFD4472 is a 20% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4472 has enhanced mold release, impact ductili.. |
|||
Flexural Modulus | 4.90 GPa | 711 ksi | ASTM D790 |
Kolon Kocetal® WH702 Reinforced Grade Acetal Copolymer
(discontinued **) Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Flexural Modulus | 4.90 - 8.32 GPa | 711 - 1210 ksi | Average value: 6.31 GPa Grade Count:4 |
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are incl.. |
|||
Flexural Modulus | 4.90 GPa @Thickness 3.20 mm |
711 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUMID GP3300B(W) PA66+MF30%, General Purpose Feature: Injection Molding, PA66+MF30%, General PurposeApplication: Automotive (Engine Cover))CAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical |
|||
Flexural Modulus | 4.90 GPa @Thickness 3.20 mm |
711 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOS GP2206F ABS+GF20%, Flame Retardant Feature: Injection Molding, ABS+GF20%, Flame RetardantApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7, 65997-17-3, 88497-56-7 and 1309-64-4Information provided b.. |
|||
Flexural Modulus | 4.90 GPa | 711 ksi | ASTM D570 |
LG Chemical Lupox® PBT-GP-2150 15% GFR PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 4.90 GPa @Thickness 3.20 mm |
711 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical Lupox® SG5150 PBT+PET+GF15% Description: Injection Molding, PBT+PET+GF15%, Good SurfaceApplication: E&E, Automotive (Door Latch)CAS No. 65997-17-3, 25038-59-9 and 24968-12-5Information provided by LG Chemical |
|||
Flexural Modulus | 4.90 GPa | 711 ksi | ASTM D790 |
IRPC Polimaxx Polene 2511HX GA5 Polypropylene Compound CHARACTERISTICS: POLYPROPYLENE BLOCK COPOLYMER WITH 25% GLASS FIBRE REINFORCED VERY HIGH IMPACT STRENGTH, HIGH MECHANICAL STRENGTH, LOW SHRINKAGE, HIGH STIFFNESS, CONTAIN UV STABILIZER AND LONG TERM.. |
|||
Flexural Modulus | 4.90 GPa | 711 ksi | ASTM D790 |
Gromax CCP ABS/PBT 7320H-104 20% Glass Fiber Filled Product Description: A 20% glass fiber reinforced injection molding grade. Characteristics:Low warp age and excellent dimensionally stable Excellent electrical property Excellent mechanic and chemi.. |
|||
Flexural Modulus | 4.90 GPa | 711 ksi | ASTM D790 |
Gromax PBT 3015-201 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Flexural Modulus | 4.90 GPa | 711 ksi | ISO 178 |
Solvay TECHNYL® C 218 V 30 PA6, 30% glass fiber, Conditioned Description: TECHNYL® C 218 V30 is a polyamide 6, heat stabilized, reinforced with 30% of glass fiber, for injection molding. This product is available in black color.Benefits: The product offers.. |
|||
Flexural Modulus | 4.90 GPa | 711 ksi | ISO 178 |
Solvay TECHNYLSTARâ„¢ S 218 V30 PA6, 30% glass filled, Conditioned Description: TECHNYLSTARâ„¢ S 218 V30 is based on a patented high flow polyamide 6 resin (TechnylStar), heat stabilized, reinforced with 30% of glass fiber, for injection molding. This product is.. |
|||
Flexural Modulus | 4.90 GPa @Temperature 175 °C |
711 ksi @Temperature 347 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr.. |
|||
Flexural Modulus | 4.90 GPa | 711 ksi | ASTM D790 |
SABIC Innovative Plastics NORYL NC208 PPE+HIPS (Asia Pacific) |
|||
Flexural Modulus | 4.90 GPa | 711 ksi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® P305G30 PP, 30% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Modulus | 4.90 GPa | 711 ksi | ISO 178-93 |
Wellman Wellamid® GF14-60 XE-NBK1 Nylon 6, 14% Glass Fiber Reinforced All information provided by Wellman Engineered Resins. |
|||
Flexural Modulus | 4.90 GPa | 711 ksi | ISO 178-93 |
Wellman Wellamid® GFT1835-WBK1 Nylon 66, 17% Glass Fiber Reinforced, Impact Modified All information provided by Wellman Engineered Resins. |
|||
Flexural Modulus | 4.90 GPa | 711 ksi | ISO 178 |
Wellman Wellamid® MR340 42H-N 34% Mineral Reinforced Nylon 6, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Flexural Modulus | 4.90 GPa @Temperature 22.8 °C |
711 ksi @Temperature 73.0 °F |
ASTM D790 |
Ensinger TECATOR™ TI 5013 Polyamide-imide (PAI) TECATOR™ is a high performance melt processable polyamideimide that maintains its excellent mechanical and wear properties in temperature environments exceeding 500°F. Stock shapes from Ensinger .. |
|||
Flexural Modulus | 4.90 GPa | 711 ksi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® 70G13HS1L BK031 Nylon 66
(Unverified Data**) 13% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G13HS1L BK031 is a 13% glass fiber reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont .. |
|||
Flexural Modulus | 4.90 GPa | 711 ksi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® 70K20HSL NC010 Nylon 66
(Unverified Data**) Kevlar® Fiber Reinforced Heat Stabilized Polyamide 66 Zytel 70K20HSL NC010 is a heat stabilized PA66 resin modified with Kevlar aramid fiber for excellent wear resistance.Information provided by Du.. |
|||
Flexural Modulus | 4.90 GPa | 711 ksi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® HTN 54G15HSLR NC010 Polyphthalamide (PPA)
(Unverified Data**) 15% Glass Reinforced Toughened PPA High Performance Polyamide Zytel HTN54G15HSLR NC010 is a 15% glass reinforced toughened heat stabilized hydrolysis resistant high performance polyamide resin. It i.. |
|||
Flexural Modulus | 4.90 GPa | 711 ksi | ASTM D790 |
Ashley Polymers Ashlene® 265 PPO, 20% Glass Reinforced A general purpose, 20% glass reinforced PPO resin for injection molding applications.Data provided by the manufacturer |
|||
Flexural Modulus | 4.90 GPa | 711 ksi | ASTM D790 |
Ashley Polymers Ashlene® 630-13G Nylon 6, 13% Glass Reinforced A 13% glass fiber reinforced Nylon 6, designed to provide a high flexural modulus and good dimensional stability, while maintaining the ease of processing associated with Nylon 6 type materials.Data.. |
|||
Flexural Modulus | 4.90 GPa | 711 ksi | ASTM D790 |
Ashley Polymers Ashlene® P123WO PBT Polyester, 15% Glass Reinforced PBT polyester with 15% glass reinforcement, flame retardant.Data provided by the manufacturer |
|||
Flexural Modulus | 4.90 GPa | 711 ksi | ASTM D790 |
Ashley Polymers Ashlene® P265WO PPO, 20% Glass Reinforced A general purpose, 20% glass reinforced flame retardant, PPO resin for injection molding applications requiring structural strength, dimensional stability and good heat resistance.Data provided by t.. |
|||
Flexural Modulus | 4.90 GPa | 711 ksi | 2.8mm/min; ASTM D790 |
Asia International Enterprise (Hong Kong) 30G3 Polybutylene terephthalate, 15% Glass Fiber Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Flexural Modulus | 4.90 GPa | 711 ksi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® C501G15 Nylon 6, 15% Glass Filled Information from Shinkong Synthetic Fibers Corp. |