Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
ASTM D5420 |
Flint Hills AP6835-HS Polypropylene Impact Copolymer Features: Excellent processing, good low temperature impact strength.Applications: Injection molding: Appliance components, consumer durables and closuresInformation Provided by Flint Hills Resource.. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 1008-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1008-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristics .. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 402 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 402 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 408 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 408 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 510 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 510 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Gardner Impact | >= 36.0 J | >= 26.6 ft-lb | |
A. Schulman POLYFORT™ PP 1498HU UV Stabilized, Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1498HU is a high flow UV stabilized medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. .. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 293 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP293 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring excellent low temperature impact properties with good dim.. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 512 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 512 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 1008-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1008-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristics .. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 403 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 403 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 504 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 504 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp.. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 512 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 512 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 608 Olefinic Elastomer DescriptionPolytrope TPP 608 is an olefinic elastomer exhibiting low thermal expansion, low heat sag and high DOI on painted parts. ApplicationTPP 608 is designed specifically for automotive fascia.. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 1008-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1008-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristics .. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 1010E-01 Olefinic Elastomer For Sheet Extrusion DescriptionPolytrope TPP 1010E-01 is an olefinic elastomer designed for sheet extrusion, profile extrusion and blow molding. TPP 1010E-01 is a natural product which can be colored and UV stabilized.. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 293 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP293 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring excellent low temperature impact properties with good dim.. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 1010-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1010-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristics .. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 503 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 503 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp.. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ CB 1010U-330 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope CB 1010U-330 is a color matched/color blended injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properti.. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 1010-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1010-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristics .. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 1010E-01 Olefinic Elastomer For Sheet Extrusion DescriptionPolytrope TPP 1010E-01 is an olefinic elastomer designed for sheet extrusion, profile extrusion and blow molding. TPP 1010E-01 is a natural product which can be colored and UV stabilized.. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ CB 1010U-330 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope CB 1010U-330 is a color matched/color blended injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properti.. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 1010-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1010-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristics .. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 402 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 402 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 510 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 510 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 508 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 508 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 293 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP293 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring excellent low temperature impact properties with good dim.. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 508 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 508 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Gardner Impact | >= 36.0 J | >= 26.6 ft-lb | |
A. Schulman POLYFORT™ PP 1498HU UV Stabilized, Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1498HU is a high flow UV stabilized medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. .. |
|||
Gardner Impact | 36.0 J | 26.6 ft-lb | ASTM D3029 |
SABIC Innovative Plastics ULTEM 1000 PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June, 2007 this grade will no longer.. |