Flint Hills P9M7R-056 Specialty Homopolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Flint Hills Resources
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Flint Hills P9M7R-056 Specialty Homopolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Clarified, e-beam and Gamma radiation sterilizable and Autoclavable. Product does not contain animal derived components. Phthalate-free.Applications: Injection molding - Lab ware, Pipette tips.Information provided by Flint Hills Resources.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 55 g/10 min
55 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 103
103
ASTM D785
Tensile Strength, Yield 33.0 MPa
4790 psi
ASTM D638
Elongation at Yield 9.5 %
9.5 %
ASTM D638
Flexural Modulus, 1% Secant 1200 MPa
174000 psi
ASTM D790
Izod Impact, Notched 0.370 J/cm
0.693 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 105 °C
221 °F
ASTM D648
Descriptive Properties Value Comments
FDA 21 CFR 177.1520(c) 1.1a
USP Class VI 88
Users viewing this material also viewed the following: