Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 230 °C |
55 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
NCMT NanoPAC™ HS402 High Performance Polypropylene Nanocomposite Applications: Electrical AppliancesInformation provided by Nano Composite Materials Technology Limited |
|||
Melt Flow | 55 g/10 min @Load 1.20 kg, Temperature 300 °C |
55 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HFD1930 PC Copolymer 55 MFR LEXAN High Flow Ductile Copolymer, Natural color only |
|||
Melt Flow | 55 g/10 min @Load 1.20 kg, Temperature 300 °C |
55 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HFD1930 PC Copolymer (Asia Pacific) 55 MFR LEXAN High Flow Ductile Copolymer, Natural color only |
|||
Melt Flow | 55 g/10 min | 55 g/10 min | ASTM D1238 |
ExxonMobil Santoprene® 912BA Thermoplastic Elastomer
(discontinued **) A hard, black, super high-flow thermoplastic olefin (TPO) in the thermoplastic elastomer (TPE) family. This grade of Vistaflex TPE is temperature-dependent and can be processed on conventional therm.. |
|||
Melt Flow | 55 g/10 min @Load 1.20 kg, Temperature 300 °C |
55 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HFD1910 PC Copolymer 55 MFR LEXAN High Flow Ductile Copolymer, Natural colors only |
|||
Melt Flow | 55 g/10 min @Load 1.20 kg, Temperature 300 °C |
55 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HFD1910 PC Copolymer (Europe-Africa-Middle East) 55 MFR LEXAN High Flow Ductile Copolymer, Natural colors only |
|||
Melt Flow | 55 g/10 min @Load 5.00 kg, Temperature 300 °C |
55 g/10 min @Load 11.0 lb, Temperature 572 °F |
|
Lehmann & Voss LUVOCOM® 50/TF/15/NAT Polycarbonate, with PTFE, easy flowing Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Melt Flow | 55 g/10 min @Load 10.0 kg, Temperature 220 °C |
55 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
LG Chemical AF312A ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Melt Flow | 55 g/10 min @Load 5.00 kg, Temperature 266 °C |
55 g/10 min @Load 11.0 lb, Temperature 511 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® 420 PBT (Europe-Africa-Middle East) VALOX 420 is a 30% glass fiber reinforced PBT injection moulding resin with excellent mechanical and thermal properties. Applications: appliance handles, spotlights, electric motors. |
|||
Melt Flow | 55 g/10 min @Load 10.0 kg, Temperature 300 °C |
55 g/10 min @Load 22.0 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics LNP STAT-KON DX07323 PC+ABS (Asia Pacific) LNP* STAT-KON* DX07323 is a compound based on polycarbonate resin containing conductive fillers. Added features of this compound includes: ESD safe and excellent low-temperature impact performance, .. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 250 °C |
55 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® ASF-9810F PBT/PET, Mineral Filled General Purpose Material for automobile lamp with high flowInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 250 °C |
55 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® ASF-9810F PBT/PET, Mineral Filled General Purpose Material for automobile lamp with high flowInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 55 g/10 min @Load 10.0 kg, Temperature 220 °C |
55 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® NH-1027HF PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 250 °C |
55 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Samyang Tribit® 1550GN15 PBT Alloy, Reinforced Flame Retardancy Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1550GN15 is a reinforced, flame retardant (.. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 230 °C |
55 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis HJ320MO Polypropylene HJ320MO is a polypropylene homopolymer intended for injection molding. Its very high melt flow makes it especially suitable for thin-wall packaging and products with long flow length. This grade is .. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 190 °C |
55 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ White L8350 HSF Concentrate Based In High-Flow LLDPE DescriptionPOLYBATCH® L8350 HSF is a specialty white color concentrate containing 50% TiO2 based in high flow LLDPE. This products stearate free and has also been designed to offer excellent dispe.. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 190 °C |
55 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ White L8350 HSF Concentrate Based In High-Flow LLDPE DescriptionPOLYBATCH® L8350 HSF is a specialty white color concentrate containing 50% TiO2 based in high flow LLDPE. This products stearate free and has also been designed to offer excellent dispe.. |
|||
Melt Flow | 55 - 60 g/10 min @Load 10.0 kg, Temperature 220 °C |
55 - 60 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Polyram RamShine PV527 Acrylonitrile Butadiene Styrene, Flame Retardant Flame retardant ABS for injection molding applications.Information provided by Polyram. |
|||
Melt Flow | 55 g/10 min @Temperature 230 °C |
55 g/10 min @Temperature 446 °F |
I<sub>2</sub>; ASTM D1238 |
Formosa Plastics Formolene® 3355E Random Copolymer Polypropylene Random Copolymer for Containers, Totes and Bins, and Closures Formolene® 3355E is a high melt flow random copolymer with fast cycle time and good mold and denesting release. It is designed for inje.. |
|||
Melt Flow | 55 g/10 min @Temperature 230 °C |
55 g/10 min @Temperature 446 °F |
I<sub>2</sub>; ASTM D1238 |
Formosa Plastics Formolene® 3355O Random Copolymer Polypropylene Random Copolymer for Clear Storage Containers and Food and Beverage Containers Formolene® 3355O is a high melt flow random copolymer with fast cycle time and easy mold release. It is designed for i.. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 230 °C |
55 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Total PPH 11012 Polypropylene Homopolymer, Injection Molding Polypropylene PPH 11012 is a nucleated controlled-rheology antistatic homopolymer with a high melt flow index of 55 g/10 min.Polypropylene PPH 11012 is characterized by high fluidity for high speed .. |
|||
Melt Flow | 55 g/10 min | 55 g/10 min | |
Toyobo GLAMIDE® T-802 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 190 °C |
55 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ White L8350 HSF Concentrate Based In High-Flow LLDPE DescriptionPOLYBATCH® L8350 HSF is a specialty white color concentrate containing 50% TiO2 based in high flow LLDPE. This products stearate free and has also been designed to offer excellent dispe.. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg |
55 g/10 min @Load 4.76 lb |
Melt flow ratio I10/I2 is 8. |
Dow LDPE 959I Low Density Polyethylene DOW LDPE 959I resin is a medium molecular weight distribution homo polymer designed to offer excellent clarity and flexibility with low warpage for lids. This resin has good processability over a wi.. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 230 °C |
55 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Carmel Olefins CAPILENE® W 77 AV Polypropylene Homopolymer CAPILENE® W 77 AV is a very high melt flow rate polypropylene homopolymer for injection molding with antistatic and nucleating additives. It offers a good balance of stiffness and flow, high de-mol.. |
|||
Melt Flow | 55 - 65 g/10 min | 55 - 65 g/10 min | ISO 1133 |
Beijing Ranger Chem BLUESTAR® 1084 PBT Can be used directly for spinning, and producing color concentrates. It can also be used for production after reinforcement & compounding.Information provided by Beijing Ranger Chemical Co. |
|||
Melt Flow | 55 g/10 min @Load 5.00 kg, Temperature 275 °C |
55 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
Azoty Tarnow™ Tarnamid® T-27 GF25 Polyamide 6 - Glass Fiber Reinforced 25% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High.. |
|||
Melt Flow | 55 g/10 min @Load 10.0 kg, Temperature 220 °C |
55 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D-1238 |
Bhansali Engineering Abstron SHF-50+ ABS Injection Molding Grade High Flow High Gloss, Fancy ApplicationsInformation provided by Bhansali |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 190 °C |
55 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ White L8350 HSF Concentrate Based In High-Flow LLDPE DescriptionPOLYBATCH® L8350 HSF is a specialty white color concentrate containing 50% TiO2 based in high flow LLDPE. This products stearate free and has also been designed to offer excellent dispe.. |