Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Formosa Plastics Formolene® 3320B Random Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Formosa Plastics Corporation, USA
Trade Name Formolene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolene® 3320B Random Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Random Copolymer for Storage Boxes, Pill Vials and Containers Formolene® 3320B is a high flow random copolymer with fast cycle time and easy mold release. It is designed for injection molding applications. Its clarity makes it an excellent choice for “see-through” housewares and rigid packaging. Formolene® 3320B meets all requirements of the U. S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles and components of articles intended for direct food contact.Specimens were injection molded according to the conditions specified in ASTM D4101Information provided by Formosa Plastics Corporation, USA
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 20 g/10 min

@Temperature 230 °C
20 g/10 min

@Temperature 446 °F
I<sub>2</sub>; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength, Yield 29.0 MPa
4200 psi
2" (50mm) per min; ASTM D638
Elongation at Yield 12 %
12 %
2" (50mm) per min; ASTM D638
Flexural Modulus 1.03 GPa
150 ksi
1.3mm per min, 1% secant; ASTM D790
Izod Impact, Notched 0.214 J/cm

@Temperature 0.000 °C
0.400 ft-lb/in

@Temperature 32.0 °F
ASTM D256
0.694 J/cm

@Temperature 23.0 °C
1.30 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 87.0 °C
189 °F
ASTM D648
Users viewing this material also viewed the following: