Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Formosa Plastics Formolene® L42009F Film (Butene Grade) LLDPE

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE)/Butene, Film
Manufacturer Formosa Plastics Corporation, USA
Trade Name Formolene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolene® L42009F Film (Butene Grade) LLDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Extra High Molecular Weight Hexene Copolymer Formolene® L42009F is a general-purpose film grade linear low density made using gas-phase technology. The resin exhibits excellent toughness and strength when drawn down to thin gauges. Formolene® L42009F meets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles intended for direct food contact.Applications: Blending Resin, Industrial Liners, Industrial Packaging, Garment Bags and Co-ExtrusionInformation provided by Formosa Plastics Corporation, USA
Physical Properties Metric English Comments
Density 0.919 g/cc
0.0332 lb/in³
ASTM D1505
Thickness 25.0 microns
0.984 mil
Melt Flow 0.95 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.95 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Condition E; ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 700 %
700 %
ASTM D882
Film Elongation at Break, TD 815 %
815 %
ASTM D882
Elmendorf Tear Strength MD 160 g
160 g
ASTM D1922
Elmendorf Tear Strength TD 400 g
400 g
ASTM D1922
Dart Drop Test 135 g
0.298 lb
ASTM D1709
Film Tensile Strength at Break, MD 35.2 MPa
5100 psi
ASTM D882
Film Tensile Strength at Break, TD 22.24 MPa
3225 psi
ASTM D882
Optical Properties Metric English Comments
Haze 27 %
27 %
ASTM D1003
Gloss 36 %
36 %
45°C; ASTM D523
Processing Properties Metric English Comments
Blow-up Ratio (BUR) 2.5
2.5
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved