Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Formosa Plastics Formolene® L62022B Film (Hexene Grade) LLDPE

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade
Manufacturer Formosa Plastics Corporation, USA
Trade Name Formolene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolene® L62022B Film (Hexene Grade) LLDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hexene Copolymer (Barefoot)Applications: Cast stretch film and high quality packaging films requiring clarity and toughness.A Hexene Copolymer Linear Low Density Polyethylene for film applications including cast stretch film and high quality packaging films requiring clarity and toughness. Available with different additive packages.Meets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles intended for direct food contact.Film properties measured on 20 micron cast film extruded at 1000 ft/min with a melt temperature at 510°F. Actual film properties may vary depending on operating conditions.Information provided by Formosa Plastics Corporation, USA.
Physical Properties Metric English Comments
Density 0.919 g/cc
0.0332 lb/in³
ASTM D1505
Thickness 20.0 microns
0.787 mil
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Condition E; ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 500 %
500 %
ASTM D882
Film Elongation at Break, TD 915 %
915 %
ASTM D882
Elmendorf Tear Strength, MD 11.6 g/micron
295 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 24.7 g/micron
628 g/mil
ASTM D1922
Dart Drop 3.66 g/micron
93.0 g/mil
ASTM D1709
Film Tensile Strength at Break, MD 44.82 MPa
6500 psi
ASTM D882
Film Tensile Strength at Break, TD 34.47 MPa
5000 psi
ASTM D882
Optical Properties Metric English Comments
Haze 1.7 %
1.7 %
ASTM D1003
Gloss 98 %
98 %
45°; ASTM D2457