Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 80.0 - 120 kN/m | 456 - 685 pli | Average value: 98.2 kN/m Grade Count:5 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO), Blow Molding Grade". Each property range of values reported is m.. |
|||
Tear Strength | 80.0 kN/m | 456 pli | Die C; ASTM D624 |
Covestro Texin® DP7-3006 Thermoplastic Polyurethane, Polyether-based, Aliphatic
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Tear Strength | 80.0 kN/m | 456 pli | Die C, 2 in/min; ASTM D1004 |
PolyOne Geon™ Vinyl Flexible 90010 Polyvinyl Chloride, Flexible (PVC, Flexible) Automotive OEM approval(s).Information provided by PolyOne |
|||
Tear Strength | 80.0 kN/m | 456 pli | ASTM D624 |
GRECO ISOTHANE 2058A Poly(caprolactone)ester TPUÂ Resin ISOTHANE 2000 series products are polyester poly(caprolactone)ester based thermoplastic polyurethane. They exhibit excellent toughness, abrasive resistance, solvent resistance, and hydrolysis stabi.. |
|||
Tear Strength | 80.0 kN/m | 456 pli | ASTM D624 |
GRECO ISOTHANE 1075A Poly(adipate)ester TPUÂ Resin ISOTHANE 1000 series products are general purpose poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance, and solvent resistance. These products .. |
|||
Tear Strength | 80.0 kN/m | 456 pli | ASTM D624 |
GRECO ISOTHANE 1080A Poly(adipate)ester TPUÂ Resin ISOTHANE 1000 series products are general purpose poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance, and solvent resistance. These products .. |
|||
Tear Strength | 80.0 kN/m | 456 pli | ASTM D624 |
GRECO ISOTHANE 1080AF Poly(adipate)ester TPUÂ Resin ISOTHANE 1000 FDA series products are poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance and solvent resistance. These products can be inject.. |
|||
Tear Strength | 80.0 kN/m | 456 pli | ASTM D624 |
GRECO ISOTHANE 1085A Poly(adipate)ester TPUÂ Resin ISOTHANE 1000 series products are general purpose poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance, and solvent resistance. These products .. |
|||
Tear Strength | 80.0 kN/m | 456 pli | ASTM D624 |
GRECO ISOTHANE 1085AF Poly(adipate)ester TPUÂ Resin ISOTHANE 1000 FDA series products are poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance and solvent resistance. These products can be inject.. |
|||
Tear Strength | 80.0 kN/m | 456 pli | ASTM D624 |
GRECO ISOTHANE 2080A Poly(caprolactone)ester TPUÂ Resin ISOTHANE 2000 series products are polyester poly(caprolactone)ester based thermoplastic polyurethane. They exhibit excellent toughness, abrasive resistance, solvent resistance, and hydrolysis stabi.. |
|||
Tear Strength | 80.0 kN/m | 456 pli | MD; ISO 6383-2 |
Iran Petrochemical (PCC) 2004TC37 Low Density Polyethylene LDPE 2004TC37: Light duty film used for very thin films requiring good optical properties for general packaging.Information provided by Iran Petrochemical Commercial Co. |
|||
Tear Strength | 80.0 kN/m | 456 pli | ASTM D624 |
A. Schulman POLYTROPE™ TPP 402 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 402 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Tear Strength | 80.0 kN/m | 456 pli | ASTM D624 |
Wanhua Chemical Wanthane® WHT-1285 Polyester Based TPU Good mechanical properties, good extrusion stability, low costInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tear Strength | 80.0 kN/m | 456 pli | ASTM D624 |
Wanhua Chemical Wanthane® WHT-8185 Polyether-Based TPU Excellent hydrolytic stability, fungus resistance, low temperature flexibility & UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tear Strength | 80.0 kN/m | 456 pli | ASTM D624 |
Wanhua Chemical Wanthane® WHT-8285 Polyether-Based TPU Excellent transparency, short cycle time, hydrolytic stability, fungus resistance, low temperature flexibility, UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tear Strength | 80.0 kN/m | 456 pli | ASTM D624 |
A. Schulman POLYTROPE™ TPP 402 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 402 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Tear Strength | 80.0 kN/m | 456 pli | ASTM D624 |
A. Schulman POLYTROPE™ TPP 402 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 402 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Tear Strength | 80.0 kN/m | 456 pli | ASTM D624 |
A. Schulman POLYTROPE™ TPP 402 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 402 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Tear Strength | 80.0 kN/m | 456 pli | ASTM D624 |
Wanhua Chemical Wanthane® WHT-1680AB Polyester Based TPU Stable melt viscosity, outstanding toughness & tear resistance, good workability for high frequency weldingInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tear Strength | 80.0 kN/m | 456 pli | DIN 53515 |
Lubrizol ESTANE® 5712F30 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 80.0 kN/m | 456 pli | DIN 53515 |
Lubrizol ESTANE® 5778 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 80.0 kN/m | 456 pli | Die C; ASTM D624 |
Covestro Bayflex® 110-35 IMR Polyurethane Elastomeric RIM, 18% Mineral Filled, MDI-based 2-Component Liquid System Calcium Silicate filled. 0.15 in. thickness. IMR=Internal Mold Release RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Ba.. |
|||
Tear Strength | 80.0 kN/m | 456 pli | Die C; ASTM D624 |
Covestro Bayflex® XGT-16 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
Tear Strength | 80.0 kN/m | 456 pli | ASTM D624 |
BASF Elastollan® 1175AW Polyether Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes... |
|||
Tear Strength | 80.0 kN/m | 456 pli | ASTM D624 |
BASF Elastollan® S80A Polyester Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan S series of products are polyester-based thermoplastic polyurethanes that exhibit good hydrolytic stability. They also exhibit good oil, fue.. |
|||
Tear Strength | >= 80.0 kN/m | >= 456 pli | ISO 34 |
Austin Novel Materials Texalan® 282A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech |
|||
Tear Strength | 80.0 kN/m | 456 pli | normal; ISO 34-1 |
DuPont Performance Polymers Hytrel® G3548 NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 35 Shore D Standard Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers |
|||
Tear Strength | 80.0 kN/m | 456 pli | ASTM D624 |
A. Schulman POLYTROPE™ TPP 402 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 402 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Tear Strength | 80.0 kN/m | 456 pli | ASTM D624 |
A. Schulman POLYTROPE™ TPP 402 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 402 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |