Garlock 505 CPE Sheet Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Chlorosulfonated Polyethylene Rubber
Manufacturer Garlock Rubber Technologies
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Garlock 505 CPE Sheet Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Style #505 is a branded, chlorinated polyethylene (CPE) sheet rubber product. CPE has excellent resistance to many chemical groups such as oils, acids, bases and alcohols. CPE is also very resistant to oxidation, heat and ozone.Information provided by Garlock Rubber Technologies
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc
1.11 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 65 - 75
65 - 75
80 - 90

@Treatment Temp. 125 °C,
Time 252000 sec
80 - 90

@Treatment Temp. 257 °F,
Time 70.0 hour
Heat Aged
Tensile Strength >= 12.4 MPa
>= 1800 psi
13.8 MPa
2000 psi
Typical
Elongation at Break >= 350 %
>= 350 %
>= 300 %

@Treatment Temp. 125 °C,
Time 252000 sec
>= 300 %

@Treatment Temp. 257 °F,
Time 70.0 hour
Heat Aged; ASTM D573
Compression Set 60 %

@Temperature 125 °C,
Time 79200 sec
60 %

@Temperature 257 °F,
Time 22.0 hour
ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 135 °C
275 °F
Minimum Service Temperature, Air -28.9 °C
-20.0 °F