Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Protective Coating PC-Clear™ Clear Liquid Epoxy PC-Clear™ is a completely clear liquid epoxy formulated to remain clear during and after its curing time. PC-Clear™ is very durable and flexible making it unlike many liquid epoxies. Uses include.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Garlock 2564 C.I. NBR/CR/SBR Sheet Rubber, Polyester Insert Garlock cloth-inserted materials are designed to add stability where mechanical fastening is necessary, and to reduce gasket creep where heavy flange loading is required.Style #2264 is a smooth fini.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Garlock 60 SBR Sheet Rubber SBR rubber specially compounded to be quick-sealing, non-hardening and heat resistant.Red, cloth finish, drum curedInformation provided by Garlock Rubber Technologies |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Garlock Bay State 22 Natural/SBR Sheet Rubber Blend of natural and SBR rubber, specially compounded to be quick-sealing, non-hardening and heat resistant.Red, smooth rotocured finish. It conforms easily to uneven flange surfaces.Information pr.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Garlock SBR Extruded Skirtboard SBR rubber extruded skirtboard for protection applicationsInformation provided by Garlock Rubber Technologies |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Garlock Super Rinohideâ„¢ 7160 SBR Rubber Lining SBR rubber lining for protection applications such as chute lining and skirtboards.Super RINOHIDEâ„¢, in particular, performs with superior resistance to abrasion, impact, aging and weathering. .. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Greene Tweed CHEMRAZ® 528 Perfluoroelastomer Chemraz® 528 works well in a wide variety of biotechnology and medical device applications where ling-term seal reliability is required. This seal material offers excellent performance in static.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | Approx. Cold test |
Lubriplate EMB Lithium-Polymer Type Grease For Special Applications / Conditions Lithium polymer type grease developed specifically for the lubrication of electric motor bearings, fans, and other high speed grease type ball and roller bearings. Applications: Electric motor beari.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Garlock 9064 Neoprene Sheet Rubber Gasketing Neoprene (CR)FDA-approved. Exceptional material for food plants, with superior resistance to most all food products; oily and aqueous.Information provided by Garlock Rubber Technologies |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Saint-Gobain CHR® 2819-3(R) Acrylic Adhesive Zone Tape Specification Notes: 21CFR177.1550 compliant. All data based on a 0.003 inch test sample.Information provided by Saint Gobain Performance Products. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Saint-Gobain CHR® C680 Paper Backing Silicone Adhesive Pressure Sensitive Tape Description: Paper tapes are designed to provide high temperature and excellent solvent resistance for wave soldering, printed circuit board masking, and hot air leveling applications. Service tempe.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Saint-Gobain CHR® K102 Polyimide Film Backing Acrylic Adhesive Pressure Sensitive Tape Description: Polyimide films are employed because of their extreme heat resistance. Service temperatures range from -100°F to 500°F (-73°C to 260°C). These flame retardant films exhibit .. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Saint-Gobain CHR® K103 Polyimide Film Backing Acrylic Adhesive Pressure Sensitive Tape Description: Polyimide films are employed because of their extreme heat resistance. Service temperatures range from -100°F to 500°F (-73°C to 260°C). These flame retardant films exhibit .. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Saint-Gobain CHR® M60 Polyester Film Backing Acrylic Adhesive Pressure Sensitive Tape Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low water absorptio.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Saint-Gobain CHR® M69 Polyester Film Backing Acrylic Adhesive Pressure Sensitive Tape Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low water absorptio.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Saint-Gobain CHR® M705 Polyester Film Backing Acrylic Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Saint-Gobain CHR® M765 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Saint-Gobain CHR® M97 Polyester Film Backing Acrylic Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Saint-Gobain CHR® M99 Polyester Film Backing Acrylic Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Saint-Gobain Tygon® LP 1100 Low Permeation Fuel Tubing Tygon® LP1100 Low Permeation Fuel Tubing is designed to meet new emission standards. Applications Lawn and garden power equipment Lubricating oil and grease transfer lines Small engine fuel.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Bostik 6384 General Purpose Characteristics EVA Glue Stick Bostik 6384 General Purpose Characteristics EVA Glue StickGeneral purpose characteristics. Bonds plastics, wood, porous materials. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Bostik 720 Low temperature EVA Glue Stick Bostik 720 Low temperature EVA Glue StickLow temperature for plastic substrates used in general or light duty applications. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Bostik 120 Wood Adhesive EVA Glue Stick Bostik 120 Wood Adhesive EVA Glue StickGood hot tack for porous substrates. Wood adhesive. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Bostik 2107 General Purpose EVA Glue Stick Bostik 2107 General Purpose EVA Glue StickGeneral purpose for porous substrates. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Bostik 2124 Flexible, Long Open Time EVA Glue Stick Bostik 2124 Flexible, Long Open Time EVA Glue StickFlexible. Long open time for most difficult substrates. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Bostik 6305 Good Heat Resistance EVA Glue Stick Bostik 6305 Good Heat Resistance EVA Glue StickGood heat resistance. Adheres to a variety of coated and uncoated board stock. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | Approx. Cold test |
Lubriplate Temp G.S. Low Lithium Based Grease For Open Gearing Lithium-based open gear grease made for all types of open gears. Available in 4 formulas for a variety of conditions and temperatures. Applications: Open gears, slides, fifth wheels, low temps. Gear.. |