Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Protective Coating PC-11® White Epoxy Paste PC-11® is a Heavy Duty-white epoxy Paste formulated by the manufacturer of PC-7.® After mixing, PC-11® can be applied to a dry, wet or underwater surface and will cure to an off white color. PC.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Protective Coating PC-Clear™ Clear Liquid Epoxy PC-Clear™ is a completely clear liquid epoxy formulated to remain clear during and after its curing time. PC-Clear™ is very durable and flexible making it unlike many liquid epoxies. Uses include.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Protective Coating PC-Fahrenheit™ High Temperature Epoxy PC-Fahrenheit™ is a hand moldable putty epoxy designed for quick emergency-type repairs formulated for increased temperatures. PC-Fahrenheit™ can be expected to outperform other putties at high te.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Garlock 135 Natural Sheet Rubber Garlock Natural Rubber Sheet is manufactured from Food and Drug Administration-approved ingredients. It is a superior, long-life sheet designed specifically for general gasketing, countertops and sk.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Garlock 2103 C.I. SBR/NBR Sheet Rubber, Polyester Insert Garlock cloth-inserted materials are designed to add stability where mechanical fastening is necessary, and to reduce gasket creep where heavy flange loading is required.Style #2103 C.I. is a smooth.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Garlock 2264 C.I. EPDM Sheet Rubber, Polyester Insert Garlock cloth-inserted materials are designed to add stability where mechanical fastening is necessary, and to reduce gasket creep where heavy flange loading is required.Style #2564 is a smooth fini.. |
|||
Minimum Service Temperature, Air | -28.9 °C @Pressure <=1.03 MPa |
-20.0 °F @Pressure <=150 psi |
|
Garlock 244 Neoprene Rubber - Commercial Grade Soft blend of neoprene, nitrile and SBR rubbers for use as bumpers, pads, and in sealing and general gasket applications. It is not recommended in applications where high oil resistance is required.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Garlock 2564 C.I. NBR/CR/SBR Sheet Rubber, Polyester Insert Garlock cloth-inserted materials are designed to add stability where mechanical fastening is necessary, and to reduce gasket creep where heavy flange loading is required.Style #2264 is a smooth fini.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Garlock 50 Natural/SBR Sheet Rubber Blend of natural and SBR rubber, specially compounded to be quick-sealing, non-hardening and heat resistant.Red, cloth finish, drum curedInformation provided by Garlock Rubber Technologies |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Garlock 7164 SBR Rubber Lining SBR rubber lining for protection applications such as chute lining and skirtboards.An optional duck fabric backing is available.Information provided by Garlock Rubber Technologies |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Garlock Bay State 22 Natural/SBR Sheet Rubber Blend of natural and SBR rubber, specially compounded to be quick-sealing, non-hardening and heat resistant.Red, smooth rotocured finish. It conforms easily to uneven flange surfaces.Information pr.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Garlock Super Rinohideâ„¢ 7160 SBR Rubber Lining SBR rubber lining for protection applications such as chute lining and skirtboards.Super RINOHIDEâ„¢, in particular, performs with superior resistance to abrasion, impact, aging and weathering. .. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Greene Tweed CHEMRAZ® 528 Perfluoroelastomer Chemraz® 528 works well in a wide variety of biotechnology and medical device applications where ling-term seal reliability is required. This seal material offers excellent performance in static.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Garlock 9122 Nitrile Sheet Rubber Gasketing Nitrile (NBR)Superior resistance to aliphatic hydrocarbons, such as oil, fuels, and many types of solvents.Information provided by Garlock Rubber Technologies |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Saint-Gobain CHR® 2829-5(R) Acrylic Adhesive Zone Tape Specification Notes: UL Guide OANZ2, File E51201, MIL-T-47012, UL510. All data based on a 0.0047 inch test sample.Information provided by Saint Gobain Performance Products. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Saint-Gobain CHR® C680 Paper Backing Silicone Adhesive Pressure Sensitive Tape Description: Paper tapes are designed to provide high temperature and excellent solvent resistance for wave soldering, printed circuit board masking, and hot air leveling applications. Service tempe.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Saint-Gobain CHR® HM430 High Modulus PTFE Film Backing Acrylic Adhesive Pressure Sensitive Tape Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Saint-Gobain CHR® K102 Polyimide Film Backing Acrylic Adhesive Pressure Sensitive Tape Description: Polyimide films are employed because of their extreme heat resistance. Service temperatures range from -100°F to 500°F (-73°C to 260°C). These flame retardant films exhibit .. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Saint-Gobain CHR® M705 Polyester Film Backing Acrylic Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Saint-Gobain CHR® M706 Polyester Film Backing Acrylic Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Saint-Gobain CHR® M765 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Saint-Gobain CHR® M97 Polyester Film Backing Acrylic Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Saint-Gobain CHR® M99 Polyester Film Backing Acrylic Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Saint-Gobain CHR® K109 Polyimide Film Backing Acrylic Adhesive Pressure Sensitive Tape Description: Polyimide films are employed because of their extreme heat resistance. Service temperatures range from -100°F to 500°F (-73°C to 260°C). These flame retardant films exhibit .. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Master Bond MB514 Hot Melt Adhesive Compound Master Bond Hot Melt MB514 is a high performance hot melt adhesive with the following key features: It is particularly suited for use on untreated surfaces of high and low density polyethylene, poly.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Bostik 2385 General Purpose EVA Glue Stick Bostik 2385 General Purpose EVA Glue StickGood general purpose bonding of paper, wood, cardboard, foam and fabrics. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Bostik 2391 Versatile, Good Hot Tack EVA Glue Stick Bostik 2391 Versatile, Good Hot Tack EVA Glue StickVersatile packaging product. Good "hot tack." |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Bostik 6323 High Performance, Long Open Time EVA Glue Stick Bostik 6323 High Performance, Long Open Time EVA Glue StickLong open time. Good adhesion to metal and plastics. High performance. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Bostik 6305 Good Heat Resistance EVA Glue Stick Bostik 6305 Good Heat Resistance EVA Glue StickGood heat resistance. Adheres to a variety of coated and uncoated board stock. |