Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Garlock 9900 Compressed Graphite Fiber Gasketing, Nitrile Binder

Category Polymer , Thermoset , Carbon Fiber/Thermoset Composite , Rubber or Thermoset Elastomer (TSE)
Manufacturer Garlock Rubber Technologies
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Garlock 9900 Compressed Graphite Fiber Gasketing, Nitrile Binder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Graphite fibers with a nitrile binder.Graphite fiber gasketing withstands extreme temperatures and pressures, as well as many chemicalsPassed Garlock Fire tests, and is ABS Fire Safe Type ApprovedLong-lasting seal - Unique manufacturing process minimizes cold flow and creep relaxation problemsIdeal for standard ANSI flanged connectors, as well as turbine crossover piping connectorsMultiple applications in power generation, chemical processing, hydrocarbon processing, and other industriesMedia: Steam, oils, grease, water, heat transfer fluidsInformation provided by Garlock Rubber Technologies
Physical Properties Metric English Comments
Density 1.76 g/cc
0.0637 lb/in³
Permeability 0.015
0.015
Gas Permeability, cc/min; DIN 3535 Part 4
Mechanical Properties Metric English Comments
Tensile Strength 12.4 MPa
1800 psi
across grain; ASTM F152
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 538 °C
1000 °F
343 °C

@Pressure 13.8 MPa
650 °F

@Pressure 2000 psi
Continuous
Minimum Service Temperature, Air -73.3 °C
-100 °F
Electrical Properties Metric English Comments
Dielectric Strength <= 0.0787 kV/mm

@Thickness 1.59 mm
<= 2.00 kV/in

@Thickness 0.0625 in
Unconditioned; ASTM D149
Descriptive Properties Value Comments
Color Mahogany
Compressibility, % 7-17
ASTM F36
Creep Relaxation, % 9
ASTM F38
Sealability ASTM F37B, ml/hr 0.1
ASTM Fuel A
0.1
Nitrogen
Copyright © lookpolymers.com All Rights Reserved