Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.76 g/cc | 0.0636 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Solef® 31008 PVDF Copolymer
(discontinued **) Key features of this grade: High Flexibility/ High Elongation/Cold Impact Resistance, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General .. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Solef® 61010 PVDF Copolymer
(discontinued **) Key features of this grade: Permanent Plasticizing, Fuel Line, Piping, Formulated. Recommended processing is extrusion. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF i.. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ISO 1183 |
Celanese VECTRA S471 LCP, 45% Mineral / Glass Reinforced
(Unverified Data**) High flow, High Heat resistance, Low Warpage, for Thick Walled (>0.2mm) or thin ( |
|||
Density | 1.76 g/cc | 0.0637 lb/in³ | |
Garlock 5500 Compressed Inorganic Fiber Gasketing, Nitrile Binder Inorganic fibers with a nitrile binder.Inorganic fiber gasketing offers excellent thermal stability with minimal weight lossReduced creep relaxation and improved torque retention provide optimal sea.. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP UX05051 PPA (Europe-Africa-Middle East) Internally lubricated Polyphthalamide compound, containing Glass Fiber and PTFE. Added features include Heat Stabilized, Flame Retardant and Hot Water Moldable |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Solef® 460/461 Polyvinylidene Fluoride (PVDF) Solef® 460/461 PVDF homopolymer has high melt viscosity and is typically processed by extrusion.Features: High Viscosity; HomopolymerAdditional Properties: Crystallization Heat - ASTM D3418 46.0 .. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ASTM D792 |
Sumitomo Bakelite North America 3-2-530 Short-Glass Reinforced Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bakelite No.. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® V8090 PBT+PET (Europe-Africa-Middle East) 50% Glass Fiber Reinforced PBT-PET resin |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp 5C003 LNP THERMOCOMP* 5C003 is a compound based on Polyvinylidene Fluoride resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. Also known as THERMOCOMP* FP-VC.. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | |
Toho Tenax Besfight® G30-500 12K HTA-7C EP01 Continuous Filament Carbon Fiber Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car.. |
|||
Density | 1.76 - 1.88 g/cc | 0.0636 - 0.0679 lb/in³ | ASTM D792 |
Zeus PVDF Tubing PVDF, polyvinylidene fluoride, delivers high performance at a competitive cost. Its inherent purity positions it as ideal for a variety of applications which involve extreme conditions. PVDF is char.. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | |
Hexcel® HexTow™ IM6 Carbon Fiber HexTow™ IM6 carbon fiber is a continuous, high performance, intermediate modulus, PAN based fiber available in 12,000 (12K) filament count tows. The fiber has been surface treated and can be sized .. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | |
Covestro Baygal® 90 IK 51 Polyurethane Uses: Suitable for the solid insulation of measuring transducers.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its ne.. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® 1SVX-65H black 9288 PA1010-GF65 Product Description: Grilamid 1SVX-65H black is a 65% glass fiber reinforced Polyamide 1010 injection molding grade with the following product profile: Raw materials based on renewable resources Exc.. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | |
Cytec Thornel® T-300 12K Carbon Fiber, Polyacrylonitrile (PAN) Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t.. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | |
Cytec Thornel® T-300 6K Carbon Fiber, Polyacrylonitrile (PAN) Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t.. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ISO 1183 |
BASF Ultradur B 4040 G10 High Speed BK15029 50% Glass Filled PBT/PET Ultradur B 4040 G10 High Speed BK15029 is a high flow, fast cycling with low warpage, 50% glass filled, injection molding PBT for industrial parts, rigid tough and dimensional stable applications. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ISO 1183 |
Celanese Vectra® A540 Liquid Crystal Polymer (LCP), 40% Mineral Filled Information provided by Celanese Corporation. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ASTM D792 |
Applied Composites 8049 Polyester SMC Industry Application: High StrengthProduct Application: MilitaryDistinct Features: High Impact Low Profile; Paintable/In Mold Coatable; Low Shrink; Low Moisture Absorption; Bondable; Formulated for .. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ISO 1183 |
3M Dyneon™ PVDF 32008/0009 Polyvinylidene Fluoride 3M™ Dyneon™ PVDF 32008/0009 is an ultra-flexible copolymer of VF2 and CTFE, exhibiting very low shrinkage and excellent impact resistance. Dyneon PVDF 32008/0009 also has a very low brittleness te.. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ISO 1183 |
Celanese VECTRA S471 LCP, 45% Mineral / Glass Reinforced High flow, High Heat resistance, Low Warpage, for Thick Walled (>0.2mm) or thin ( |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ASTM D792 |
Applied Composites 120 Polyester SMC Industry Application: ElectricalProduct Application: Transmission ProductDistinct Features: Pigmentable UL 94 V-5, Stable @ 600 Hour QUV Accelerated Weather Testing, Passed 6 Mos. AZ Outdoor Weather.. |
|||
Density | 1.76 - 1.96 g/cc | 0.0636 - 0.0708 lb/in³ | Molded |
Bulk Molding Compounds BMC HT12-1027 Unsaturated Polyester Bulk Molding Compound BMC HT12-1027 is a highly engineered Unsaturated Polyester Bulk Molding Compound developed for automotive under-hood applications. This compound is specified by Ford motor company for solenoid caps.. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ISO 1183 |
3M Dyneon™ PVDF 31508/0001 Polyvinylidene Fluoride
(discontinued **) Copolymer of VF2 and CTFEUltra-flexibleVery low shrinkage ratesWide operating temperature windowProcessable using a variety of thermoplastic conversation techniquesInformation provided by Dyneon, A .. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ISO 1183 |
3M Dyneon™ PVDF 32008/0003 Polyvinylidene Fluoride
(discontinued **) Copolymer of VF2 and CTFEUltra-flexibleVery low shrinkage ratesWide operating temperature windowProcessable using a variety of thermoplastic conversion techniquesExcellent low flame and low smoke pe.. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ISO 1183 |
3M Dyneon™ PVDF 31508/0009 Polyvinylidene Fluoride 3M™ Dyneon™ PVDF 31508/0009 is a flexible copolymer of VF2 and CTFE, exhibiting very low shrinkage and excellent impact resistance. Dyneon PVDF 31508/0009 also has a very low brittleness temperatu.. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® HTN FR52G45BL BK337 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFR52G45BL BK337 is a 45% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont .. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ISO 1183 |
3M Dyneon™ PVDF 31008/0003 Polyvinylidene Fluoride
(discontinued **) 3M™ Dyneon™ PVDF 31008/0003 is a flexible copolymer of VF2 and CTFE, exhibiting very low shrinkage and excellent impact resistance. Dyneon PVDF 31008/0003 also has a very low brittleness temperatu.. |