Glastic GLASGUARD 1130 Corrosion-Resistant Panels

Category Polymer , Thermoset , Composite SMC , Filled/Reinforced Thermoset , Polyester, TS
Manufacturer Glastic
Trade Name GLASGUARD
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Glastic GLASGUARD 1130 Corrosion-Resistant Panels.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
GlasGuard Grade 1130 is a fiberglass-reinforced thermoset polymer composite system which is available as sheet stock or in a variety of pultruded shapes. Grade 1130 possesses flame resistance, corrosion resistance, weatherability, and dielectric properties. This material meets NEMA criteria for grade GPO-3. Grade 1130 was developed to meet the requirements of the NYC Transit Authority. It has been pultruded into channel shaped covers for the electrified third rail and molded into flat panels for both a sign material and switchgear components. Information provided by Glastic Corporation
Physical Properties Metric English Comments
Water Absorption 0.10 %
0.10 %
% by wt.; ASTM D-570
Mechanical Properties Metric English Comments
Tensile Strength, Yield 101 MPa
14600 psi
Lengthwise; ASTM D-638
110 MPa
16000 psi
Crosswise; ASTM D-638
Tensile Modulus 10.3 GPa
1490 ksi
Lengthwise/Crosswise; ASTM D-638
Flexural Strength 141 MPa
20400 psi
Lengthwise; ASTM D-790
161 MPa
23300 psi
Crosswise; ASTM D-790
Flexural Modulus 9.58 GPa
1390 ksi
Crosswise; ASTM D-790
9.72 GPa
1410 ksi
Lengthwise; ASTM D-790
Adhesive Bond Strength 42.1 MPa
6100 psi
lbs.; NEMA 11.11
Izod Impact, Notched 6.03 J/cm
11.3 ft-lb/in
ASTM D-256
Thermal Properties Metric English Comments
Flammability, UL94 V-0
V-0
Flame Spread Index 12
12
Radiant Panel; ASTM E-162
20
20
UL Standard 723; ASTM E-84
Electrical Properties Metric English Comments
Dielectric Strength 12.4 kV/mm
315 kV/in
Perpendicular S/T in Air; ASTM D-149
Arc Resistance 192 sec
192 sec
ASTM D-495
Track Resistance 52200 sec
52200 sec
Inclined Plane; ASTM D-2303
Descriptive Properties Value Comments
Electric Strength kV, ASTM D149 75
Parallel, Condition A
79
Parallel, Condition D (48/50)
Smoke Developed 115
ASTM E-84
Standard Color Gray
UL Recognition File Number R9599
UL Standard 723 Fuel Contributed 0
ASTM E-84