Material Notes:
Information provided by Global Polymers Corporation.
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ASTM D792
Melt Flow 1.0 g/10 min

@Load 1.05 kg,
Temperature 190 °C
1.0 g/10 min

@Load 2.31 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 94
94
ASTM D785
Tensile Strength, Yield 69.0 MPa
10000 psi
ASTM D638
Elongation at Break 75 %
75 %
ASTM D638
Flexural Yield Strength 99.0 MPa
14400 psi
ASTM D790
Flexural Modulus 2.90 GPa
421 ksi
ASTM D790
Izod Impact, Notched 1.23 J/cm
2.30 ft-lb/in
ASTM D256
0.960 J/cm

@Temperature -40.0 °C
1.80 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D256
Tensile Impact Strength 358 kJ/m²
170 ft-lb/in²
ASTM D1822