Gouda Vuurvast CURAS 85 PD REPAIR Moldable Refractory Material

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Gouda Vuurvast
Trade Name CURAS
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast CURAS 85 PD REPAIR Moldable Refractory Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Curas 85 PD Repair is a phosphate bonded moldable based on sintered bauxite. It has been specially developed for aluminum melting and holding furnaces. However, it can be applied on any location that needs repair with a highly refractory material that has high strength over the full temperature range. Curas 85 PD Repair is supplied as a dry powder and has to be mixed with potable water to the required consistency.Remarks: The stated chemical composition and physical properties represent average values.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.70 - 2.80 g/cc
0.0975 - 0.101 lb/in³
After drying at 110°C
Thermal Properties Metric English Comments
Thermal Conductivity 0.850 - 0.950 W/m-K

@Temperature 100 °C
5.90 - 6.59 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.930 - 1.13 W/m-K

@Temperature 600 °C
6.45 - 7.84 BTU-in/hr-ft²-°F

@Temperature 1110 °F
1.23 - 1.43 W/m-K

@Temperature 1300 °C
8.54 - 9.92 BTU-in/hr-ft²-°F

@Temperature 2370 °F
Maximum Service Temperature, Air 1600 °C
2910 °F
Shrinkage -0.200 - 0.200 %

@Temperature 1300 °C
-0.200 - 0.200 %

@Temperature 2370 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 82 %
82 %
SiO2 13 %
13 %
Descriptive Properties Value Comments
Bonding Type chemical/ceramic
Material Consumption per 1 m3 2700 kg
Mixing Water 5-7 liters
per 100 kgs dry material
Segercone 37