Polymer Property : Thermal Conductivity = 7.84 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.930 - 1.13 W/m-K

@Temperature 600 °C
6.45 - 7.84 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURAS 85 PD REPAIR Moldable Refractory Material
Description: Curas 85 PD Repair is a phosphate bonded moldable based on sintered bauxite. It has been specially developed for aluminum melting and holding furnaces. However, it can be applied on any..
Thermal Conductivity 0.930 - 1.13 W/m-K

@Temperature 600 °C
6.45 - 7.84 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURAS 90 SPF Moldable Refractory Material
Description: Curas 90 S PF is a moldable which is characterized by its outstanding abrasion resistance (acc. to ASTM C-704: < 3 cc). This material is supplied as a powder which only has to be mixed ..
Thermal Conductivity 1.03 - 1.13 W/m-K

@Temperature 1300 °C
7.15 - 7.84 BTU-in/hr-ft²-°F

@Temperature 2370 °F
Gouda Vuurvast CURON 14 S Dense Refractory Castable
Description: Curon 14 S is a dense, strong and abrasion resistant castable. Because of the very low percentage of Fe2O3 and SiO2 it is used for highly abrasive conditions in reducing atmospheres.Rem..