Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 1.00 - 2.00 MPa @Temperature 100 °C |
145 - 290 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast GOLITE 125 R GM Refractory Insulating Castable Description: Golite 125 R GM has a low Fe2O3 content and a very low density. Commonly used in reducing conditions in the petrochemical industry.Remarks: These values apply to cast products.Informati.. |
|||
Compressive Strength | 1.00 - 2.00 MPa @Temperature 1000 °C |
145 - 290 psi @Temperature 1830 °F |
Cold Crushing Strength |
Gouda Vuurvast GOLITE 125 R GM Refractory Insulating Castable Description: Golite 125 R GM has a low Fe2O3 content and a very low density. Commonly used in reducing conditions in the petrochemical industry.Remarks: These values apply to cast products.Informati.. |
|||
Compressive Strength | 1.00 - 5.00 MPa @Temperature 1260 °C |
145 - 725 psi @Temperature 2300 °F |
Cold Crushing Strength |
Gouda Vuurvast GOLITE 135 L Refractory Insulating Castable Description: Golite 135 L can be used in direct contact with fire and combines a good strength with a high insulation value.Remarks: These values apply to cast products. Also available in gunning va.. |