Gwent Electronic Materials C2040226D2 Curable Carbon Ink

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Gwent Electronic Materials Ltd.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gwent Electronic Materials C2040226D2 Curable Carbon Ink.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This product is based on a unique curing process that results in the low temperature formation of a thermosetting conductive coating that combines good adhesion with excellent chemical, solvent and abrasion resistance. It offers the advantage of a One-Pak cure system combined with the convenience of Ambient Temperature stability, which means they do not have to be stored in a freezer or refrigerator.General Purpose GradeInformation provided by Gwent Electronic Materials Ltd.
Physical Properties Metric English Comments
Particle Size <= 5.0 µm
<= 5.0 µm
Fineness of Grind
Viscosity 5200 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
5200 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake Viscosity
Thickness 20.0 - 30.0 microns
0.787 - 1.18 mil
Electrical Properties Metric English Comments
Surface Resistivity per Square <= 150 ohm
<= 150 ohm
cured; 25 microns thick
Processing Properties Metric English Comments
Cure Time 30.0 - 60.0 min

@Temperature 90.0 °C
0.500 - 1.00 hour

@Temperature 194 °F
Descriptive Properties Value Comments
Coverage cm2/g 295
200 mesh stainless steel screen
Printing Mesh counts/inch 180 to 340
stainless steel or polyester screens