Material Notes:
C60531D1 has a ratio of Silver to Silver Chloride of 90/10. This is used for reference electrodes in Medical Diagnostics, Environmental Sensor and the "Agri-Food" Industries. It forms part of a family of reference electrode materials with ratios from 40/60 through 90/10 Silver/Silver Chloride.The paste is in a ready to use form at a viscosity suitable for automatic or semiautomatic screen printing. The paste should be gently stirred before use avoiding introduction of air bubbles. It is a Polymer System for printing on polyester, PVC, Polycarbonate etc and on alumina.Information provided by Gwent Electronic Materials Ltd.
Physical Properties Metric English Comments
Viscosity 3900 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
3900 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake Viscosity
Thickness 17.0 microns
0.669 mil
when printed through a 156 mesh
Storage Temperature 20.0 °C
68.0 °F
in a sealed pot
Electrical Properties Metric English Comments
Surface Resistivity per Square 0.20 ohm
0.20 ohm
cured film; 17 microns thick
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 80.0 °C
0.167 hour

@Temperature 176 °F
30.0 min

@Temperature 60.0 °C
0.500 hour

@Temperature 140 °F
Shelf Life 3.00 Month
3.00 Month
Descriptive Properties Value Comments
Coverage cm2/g 185
156 mesh polyester mesh screen with 13 micron emultion back off
Printing Mesh counts/inch 120 to 200
typical screen size is 156 Polyester