Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

H.C. Starck Amperit® 155.093 Titanium (Ti)

Category Metal , Nonferrous Metal , Pure Element
Manufacturer H.C. Starck
Trade Name Amperit®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF H.C. Starck Amperit® 155.093 Titanium (Ti).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HS Number: 81081010
Physical Properties Metric English Comments
Particle Size 125 µm
125 µm
Maximum of 10% greater than
Component Elements Properties Metric English Comments
Aluminum, Al <= 0.10 %
<= 0.10 %
Chromium, Cr <= 0.10 %
<= 0.10 %
Hydrogen, H <= 0.10 %
<= 0.10 %
Iron, Fe <= 0.30 %
<= 0.30 %
Magnesium, Mg <= 0.20 %
<= 0.20 %
Manganese, Mn <= 0.10 %
<= 0.10 %
Nitrogen, N <= 0.10 %
<= 0.10 %
Oxygen, O <= 0.40 %
<= 0.40 %
Silicon, Si <= 0.10 %
<= 0.10 %
Users viewing this material also viewed the following: