H.C. Starck Amperit® 335.063 Nickel Self-fluxing Alloy HRC 60 (NiCrBSi)

Category Metal , Nonferrous Metal , Nickel Alloy
Manufacturer H.C. Starck
Trade Name Amperit®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF H.C. Starck Amperit® 335.063 Nickel Self-fluxing Alloy HRC 60 (NiCrBSi).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Apparent Bulk Density 3.80 - 4.60 g/cc
0.137 - 0.166 lb/in³
ASTM B212
Particle Size 45 µm
45 µm
Maximum of 20% less than
75 µm
75 µm
Maximum of 5% greater than
Mechanical Properties Metric English Comments
Hardness, Rockwell C 60
60
Component Elements Properties Metric English Comments
Boron, B 2.75 - 3.5 %
2.75 - 3.5 %
Carbon, C 0.60 - 1.2 %
0.60 - 1.2 %
Nickel, Ni 67.3 - 76.65 %
67.3 - 76.65 %
Silicon, Si 4.0 - 5.0 %
4.0 - 5.0 %